Molecular Design and Acid-Heat Synergistic Aging Mechanism of Silicone Adhesives with 500 ℃ Heat Resistance

Yaosheng Liang

Ingegneria Sismica · 30.04.2026 · 42 (4) · 1-19

DOI: 10.65102/is20261015 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Ingegneria Sismica, online erschienen am 30.04.2026. Verfasst von Yaosheng Liang.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

For solving the problem that adhesive layers have early damage in hot-end sensor package, metal-ceramic connection, and heat-resisting insulation connection when they touch acid medium and discontinuous heat, this paper puts forward a kind of organosilicon adhesive system which has many phenyl groups, can be solidified through vinyl groups, and includes zirconium coordination nodes. The study investigates the mechanism underlying its 500 ℃ heat resistance and its acid-heat synergistic aging behavior. Using phenyltriethoxysilane, methyltriethoxysilane, and vinyltriethoxysilane as copolymerization monomers. Through controlled hydrolytic condensation, a phenylated siloxane prepolymer retaining a certain amount of Si-OH groups was prepared. Acetone-coordinated n-propanol zirconium was then introduced to construct Si-O-Zr nodes, yielding five formulations (P0-P4). Free-standing films and lap joints were prepared using a PMHS/Pt addition curing system. A synergistic aging protocol consisting of one cycle of "8 h acid immersion at 80 ℃+4 h heat treatment at 250 ℃" was established to characterize the chemical structure, thermal stability, post-heat bonding strength, interfacial evolution, and residual phase formation. The results indicate that P3 exhibits the best comprehensive performance under conditions of Ph/Si=0.40 and Zr/Si=0.06. This formulation had a double bond conversion rate of 93.8%, with 5% and 10% weight loss temperatures reaching 438 ℃ and 476 ℃, respectively; the residual carbon content at 800 ℃ was 56.8%, and the lap shear strength at room temperature was 8.54 MPa, which remained at 2.73 MPa after 30 minutes of thermal exposure at 500 ℃. After 15 cycles of synergistic aging, P3 retained 59.2% of its initial strength, with a synergy factor of 1.18, lower than the 1.34 for P0 and 1.29 for P1. The phenyl group increased the proportion of the high-temperature residual phase, while the Si-O-Zr nodes delayed the main weight loss zone and promoted the formation of a continuous Si/O/Zr-enriched layer on the surface; the acidic medium preferentially induces Si-O-Si hydrolysis and silanol enrichment at the surface and interface defects; the subsequent thermal phase further triggers re-condensation, oligomer escape, and volume shrinkage, ultimately manifesting as outer-layer hardening, increased modulus gradient, and expansion of the interfacial gap. This paper presents a formulation window and an acid-thermal coupled failure map applicable to thermal exposure conditions at 500 ℃.

Zitieren

APA

Liang, Y. (2026). Molecular Design and Acid-Heat Synergistic Aging Mechanism of Silicone Adhesives with 500 ℃ Heat Resistance. Ingegneria Sismica, 42(4), 1-19. https://doi.org/10.65102/is20261015

Vancouver

Liang Y. Molecular Design and Acid-Heat Synergistic Aging Mechanism of Silicone Adhesives with 500 ℃ Heat Resistance. Ingegneria Sismica. 2026;42(4):1-19. doi:10.65102/is20261015

BibTeX
@article{Liang2026,
  author = {Liang, Yaosheng},
  title = {Molecular Design and Acid-Heat Synergistic Aging Mechanism of Silicone Adhesives with 500 ℃ Heat Resistance},
  journal = {Ingegneria Sismica},
  year = {2026},
  volume = {42},
  number = {4},
  pages = {1--19},
  doi = {10.65102/is20261015}
}
Kostenlos starten →