Abstract (Originalsprache)

Lightweight concrete is currently widely used for constructing walls and partitions in urban buildings. The quality of lightweight concrete is determined by several factors, including weight or mass, water absorption, and flexural strength. This study aims to determine the optimal volume of foam agent for manufacturing Cellular Lightweight Concrete (CLC). This study employed an experimental method with a Randomized Block Design (RBD) consisting of 5 treatment levels of foam agent volume: P1 (8.5 ml), P2 (10 ml), P3 (11.5 ml), P4 (13 ml), and P5 (14.5 ml), with each treatment level replicated 3 times. The parameters analyzed were CLC weight, water absorption, and flexural strength. Data were analyzed using the F-test and the Least Significant Difference (LSD) test, followed by correlation and regression analyses. The results of the analysis of variance (ANOVA) showed that the foam agent volume treatment significantly affected the weight, water absorption, and flexural strength of the resulting CLC. The analysis revealed a negative correlation between the CLC weight and the foam agent volume, indicating a polynomial relationship. Water absorption was positively correlated with the foam agent volume, showing a positive non-linear polynomial relationship expressed by the equation Wa=0,321fa2 -3,2498fa+28,726. Furthermore, the flexural strength was negatively correlated with the foam agent volume. The 10 ml volume treatment (P2) yielded the best lightweight concrete based on considerations of CLC weight, water absorption, and flexural strength. In the production of CLC to achieve good physical and mechanical qualities, it is recommended to add 10 ml of foam agent.

Zitieren

APA

Kevin, C., & K.H, I. (2026). Penentuan Volume Foam Agent pada Pembuatan CLC (Cellular Lightweight Concrete). Agricultural Technology Sphere and Engineering Journal, 2(1), 46-52. https://doi.org/10.64723/atsej.v2i1.23

Vancouver

Kevin C, K.H I. Penentuan Volume Foam Agent pada Pembuatan CLC (Cellular Lightweight Concrete). Agricultural Technology Sphere and Engineering Journal. 2026;2(1):46-52. doi:10.64723/atsej.v2i1.23

BibTeX
@article{Kevin2026,
  author = {Kevin, Carlo and K.H, Iskandar},
  title = {Penentuan Volume Foam Agent pada Pembuatan CLC (Cellular Lightweight Concrete)},
  journal = {Agricultural Technology Sphere and Engineering Journal},
  year = {2026},
  volume = {2},
  number = {1},
  pages = {46--52},
  doi = {10.64723/atsej.v2i1.23}
}
Kostenlos starten →