Flexural and compressive strength of bis-acryl, polymethyl methacrylate, and 3D-printed provisional resins: a comparative in vitro study

Valerie Saldaña-Carranza

TUMI Oral Health · 30.06.2026 · 1 (3) · e004

DOI: 10.64716/ahbxdg78 ↗

Kurz gefasst

Fachartikel in der Zeitschrift TUMI Oral Health, online erschienen am 30.06.2026. Verfasst von Valerie Saldaña-Carranza. Die Arbeit nennt 22 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0).

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Background

Provisional restorations must maintain adequate mechanical integrity during treatment, particularly when subjected to bending and occlusal forces.

Objective

To compare the flexural and compressive strengths of a bis-acryl resin, an autopolymerizing polymethyl methacrylate (PMMA) resin, and a 3D-printed provisional resin.

Methods

A comparative experimental in vitro study was conducted using 54 specimens, with 18 specimens assigned to each material. For each group, nine specimens were evaluated for flexural strength and nine for compressive strength. After storage in distilled water at 37 °C for 24 hours, flexural strength was assessed using a three-point bending test and compressive strength by axial loading in a universal testing machine.

Results

Significant differences were found among the materials for flexural strength (F = 6.104; p = 0.007) and compressive strength (F = 20.750; p = 0.000). The bis-acryl resin showed the highest mean flexural strength (69.46 ± 7.70 MPa), followed by the 3D-printed resin (60.92 ± 3.54 MPa) and PMMA (57.04 ± 10.36 MPa). It also showed the highest mean compressive strength (82.25 ± 14.79 MPa), followed by the 3D-printed resin (75.96 ± 5.62 MPa) and PMMA (51.30 ± 9.89 MPa). Flexural strength differed significantly between the bis-acryl resin and both PMMA and the 3D-printed resin, whereas compressive strength differed significantly between PMMA and the other two materials.

Conclusion

Under the conditions of this study, the bis-acryl resin demonstrated the most favorable overall mechanical performance, while the 3D-printed resin showed compressive strength comparable to that of the bis-acryl resin.

Zitieren

APA

Saldaña-Carranza, V. (2026). Flexural and compressive strength of bis-acryl, polymethyl methacrylate, and 3D-printed provisional resins: a comparative in vitro study. TUMI Oral Health, 1(3), e004. https://doi.org/10.64716/ahbxdg78

Vancouver

Saldaña-Carranza V. Flexural and compressive strength of bis-acryl, polymethyl methacrylate, and 3D-printed provisional resins: a comparative in vitro study. TUMI Oral Health. 2026;1(3):e004. doi:10.64716/ahbxdg78

BibTeX
@article{SaldaaCarranza2026,
  author = {Saldaña-Carranza, Valerie},
  title = {Flexural and compressive strength of bis-acryl, polymethyl methacrylate, and 3D-printed provisional resins: a comparative in vitro study},
  journal = {TUMI Oral Health},
  year = {2026},
  volume = {1},
  number = {3},
  pages = {e004},
  doi = {10.64716/ahbxdg78}
}
Kostenlos starten →