Enhancing Critical Cracking Thickness of TiO₂ Films through Evaporation-Driven GME in Non-Volatility Butanediol–Water Mixtures
Chemical Technology and Engineering Applications · 2026
DOI: 10.64229/safkc237 ↗Kurz gefasst
Fachartikel in der Zeitschrift Chemical Technology and Engineering Applications, 2026. Verfasst von Juang Bhakti Hastyadi. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0).
Abstract (Originalsprache)
We report a systematic investigation of GME (1-glyceryl monooleyl ether) self-assembly of TiO₂–water–butanediol quaternary colloidal suspensions and its consequences for crack formation during film drying. Because 1,4-butanediol has a boiling point of ~230°C and a vapour pressure orders of magnitude below that of water, drying progressively enriches the GME–butanediol–water phase in both co-solvent and surfactant rather than depleting it of a volatile additive. Cross-polarised optical microscopy (POM) established that lamellar or hexagonal lyotropic liquid-crystalline (LC) phases form at ≥2 wt% GME in butanediol:water 1:20 mixtures, and at ≥2 wt% GME in 3:7 mixtures. UNIFAC-based drying-path simulations confirmed that water evaporates preferentially, predicting that 3:7 BDO/H₂O formulations at ≥2 wt% GME cross into the lamellar LC window when ≈72 ± 4% of the initial water remains. Critical cracking thickness (hᴄᴄᴛ) measurements on TiO₂ films (≈200 nm, 3.5 vol%) demonstrated a 2.3-fold increase from 17.5 ± 0.6 µm (additive-free control) to 41.4 ± 2.9 µm at 3:7 BDO/3 wt% GME at 25°C (p < 0.001, one-way ANOVA). The enhancement is primarily LC-mediated: the apparent shear modulus Gₐₚₚ of the LC phase (exp(0.71ϕf)) elevates the Tirumkudulu–Russel fracture-resistance prefactor by a factor of ≈1.7× (model R² = 0.993). Residual butanediol in dried films (9.4 ± 0.6 wt% at the 3:7/2 wt% GME condition) contributes a secondary plasticisation effect (r² = 0.62 vs. r² = 0.91 for the LC contribution). Isomer comparison confirmed that 1,4-butanediol (hᴄᴄᴛ = 34.0 µm) outperforms 1,3-butanediol (29.7 µm) and 2,3-butanediol (27.2 µm), consistent with the linear backbone geometry of 1,4-BDO favouring GME lamellar packing. These results demonstrate a low-volatility, low-VOC additive route to crack-free thick particulate coatings and offer a mechanistic framework for non-volatile co-solvent–amphiphile systems in particulate film drying.
Zitieren
APA
Hastyadi, J. B. (2026). Enhancing Critical Cracking Thickness of TiO₂ Films through Evaporation-Driven GME in Non-Volatility Butanediol–Water Mixtures. Chemical Technology and Engineering Applications. https://doi.org/10.64229/safkc237
Vancouver
Hastyadi JB. Enhancing Critical Cracking Thickness of TiO₂ Films through Evaporation-Driven GME in Non-Volatility Butanediol–Water Mixtures. Chemical Technology and Engineering Applications. 2026. doi:10.64229/safkc237
BibTeX
@article{Hastyadi2026,
author = {Hastyadi, Juang Bhakti},
title = {Enhancing Critical Cracking Thickness of TiO₂ Films through Evaporation-Driven GME in Non-Volatility Butanediol–Water Mixtures},
journal = {Chemical Technology and Engineering Applications},
year = {2026},
doi = {10.64229/safkc237}
}