PET Accelerates the Decomposition of HDPE During Co-Pyrolysis: A Non-Additive Interaction from Thermogravimetry to Bench Scale
Green and Sustainable Environments · 19.11.2026 · 1 (2)
DOI: 10.62755/gsenv.2026.10 ↗Kurz gefasst
Fachartikel in der Zeitschrift Green and Sustainable Environments, online erschienen am 19.11.2026. Verfasst von Aulia Annas Mufti und 3 weiteren Autor:innen. Die Arbeit nennt 42 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0).
Abstract (Originalsprache)
Post-consumer polyolefin waste sent to pyrolysis commonly carries poly(ethylene terephthalate) (PET), yet yield and kinetic models for such feeds often treat their components as decomposing independently. We tested that assumption by comparing the thermogravimetric response of blends of high-density polyethylene (HDPE) and PET with the mass-weighted sum of the pure polymers measured in the same campaign, in single runs at 10, 20 and 50 % PET. All blends lost mass faster than the additive prediction, by 19 %–41 % of the initial mass between 400 °C and 500 °C, and the sign of the deviation held in two campaigns run a month apart at 9.8 °C min−1 and 20.3 °C min−1, although the ranking of the blends did not. Evolved-gas analysis placed the volatile maximum of every blend within 5 °C of HDPE, but the aliphatic channel (m/z 57) of the blends left the baseline 14 °C–24 °C below that of HDPE, against a repeatability of 2 °C. Micro-pyrolysis at 600 °C gave aromatics and acids at 0.9 %–11.4 % of the identified product area for blends with 10 to 50 % PET, against 50.4 % for PET alone. In a horizontal tube reactor, a 90:10 HDPE:PET feed held for 60 min at 450 °C–550 °C gave 83 %–88 % wax and at most 5.1 % GC-quantifiable liquid, with mass balances closing to 92 %–95 %. Without a pure-HDPE reactor run, this slate cannot be assigned to PET. The additive superposition of pure-polymer curves therefore underestimates how early a PET-bearing polyolefin feed loses mass, and the evolved-gas profiles show that this earlier loss includes an earlier onset of the polyolefin fraction.
Zitieren
APA
Mufti, A. A., Palapa, N. R., Arif, M. F., & Taher, T. (2026). PET Accelerates the Decomposition of HDPE During Co-Pyrolysis: A Non-Additive Interaction from Thermogravimetry to Bench Scale. Green and Sustainable Environments, 1(2). https://doi.org/10.62755/gsenv.2026.10
Vancouver
Mufti AA, Palapa NR, Arif MF, Taher T. PET Accelerates the Decomposition of HDPE During Co-Pyrolysis: A Non-Additive Interaction from Thermogravimetry to Bench Scale. Green and Sustainable Environments. 2026;1(2). doi:10.62755/gsenv.2026.10
BibTeX
@article{Mufti2026,
author = {Mufti, Aulia Annas and Palapa, Neza Rahayu and Arif, Muhamad F. and Taher, Tarmizi},
title = {PET Accelerates the Decomposition of HDPE During Co-Pyrolysis: A Non-Additive Interaction from Thermogravimetry to Bench Scale},
journal = {Green and Sustainable Environments},
year = {2026},
volume = {1},
number = {2},
doi = {10.62755/gsenv.2026.10}
}
EUVIMED