EUVIMEDEUVIMED entdecken
Crossref

Zirconia versus lithium disilicate crown fracture resistance

Manish Sinha

Bioinformation · 30.11.2026 · 22 (11) · 8703-8708

DOI: 10.6026/973206300228703 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Bioinformation, online erschienen am 30.11.2026. Verfasst von Manish Sinha.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Monolithic ceramic crowns permit conservative tooth preparation, but their fracture resistance may vary by material and occlusal thickness. Hence, 60 standardized mandibular first-molar dies received CAD/CAM-fabricated monolithic zirconia or lithium disilicate crowns of 0.8, 1.0, or 1.5 mm occlusal thickness (n = 10 per group), followed by 10,000 thermocycles and 1.2 million mechanical cycles before loading to fracture. Mean fracture loads for zirconia were 2228 +/- 278, 2744 +/- 315 and 3612 +/- 402 N at the three thicknesses, respectively, compared with 1176 +/- 196, 1568 +/- 223 and 2194 +/- 287 N for lithium disilicate. Material and thickness significantly influenced fracture resistance (both p < 0.001), with a significant interaction (p = 0.032) and catastrophic failure was more frequent among thinner lithium disilicate crowns. Thus, zirconia had higher fracture resistance at every thickness, while increased occlusal thickness improved load-bearing capacity for both materials.

Zitieren

APA

Sinha, M. (2026). Zirconia versus lithium disilicate crown fracture resistance. Bioinformation, 22(11), 8703-8708. https://doi.org/10.6026/973206300228703

Vancouver

Sinha M. Zirconia versus lithium disilicate crown fracture resistance. Bioinformation. 2026;22(11):8703-8708. doi:10.6026/973206300228703

BibTeX
@article{Sinha2026,
  author = {Sinha, Manish},
  title = {Zirconia versus lithium disilicate crown fracture resistance},
  journal = {Bioinformation},
  year = {2026},
  volume = {22},
  number = {11},
  pages = {8703--8708},
  doi = {10.6026/973206300228703}
}
Kostenlos starten →