Push-out bond strength of zinc oxide eugenol sealer, bioceramic sealer and bioactive glass sealer to dentin among heat generated thermoplasticized gutta-percha technique

Ayushi Upadhayay, Pankaj Mishra, Santosh Kumar Singh, Shubhashree Rajput, Ashee Jain, Kehkashan Sheikh

Bioinformation · 30.06.2026 · 22 (6) · 3624-3628

DOI: 10.6026/973206300223624 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Bioinformation, online erschienen am 30.06.2026. Verfasst von Ayushi Upadhayay und 5 weiteren Autor:innen. Beteiligte Einrichtung: Department of Conservative Dentistry and Endodontics, People's College of Dental Sciences and Research Centre, People's University, Bhopal, Madhya Pr…. Der Volltext ist frei in PubMed Central verfügbar.

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Heat produced during thermoplasticized obturation negatively impacts root canal sealers, compromising their adhesion to dentin and ultimately affecting the integrity of the seal. Therefore, it is of interest to assess the push-out bond strength of zinc oxide eugenol sealer, bioceramic sealer and bioactive glass sealer following thermoplasticized gutta-percha obturation. Sixty single-rooted premolars were randomly divided into three groups and samples from the apical, middle and cervical thirds were evaluated using universal testing equipment. Hence, the bioactive glass sealer showed the greatest push-out bond strength, followed by the bioceramic sealer, whereas the zinc oxide eugenol sealer revealed the lowest values. In all three groups, the apical third consistently exhibited higher bond strength than the middle and cervical thirds. Thus, data shows the performance of traditional and contemporary sealers during heat-assisted obturation and support the potential benefits of bioactive components in enhancing sealer-dentin adhesion.

Schlagwörter

Stichwörter der Autor:innen

Push-out bond strengthbioactive glass sealerbioceramic sealerthermoplasticized gutta-perchazinc oxide eugenol sealer

Autor:innen und Institutionen

  • Department of Conservative Dentistry and Endodontics, People's College of Dental Sciences and Research Centre, People's University, Bhopal, Madhya Pradesh, India.

Zitieren

APA

Upadhayay, A., Mishra, P., Singh, S. K., Rajput, S., Jain, A., & Sheikh, K. (2026). Push-out bond strength of zinc oxide eugenol sealer, bioceramic sealer and bioactive glass sealer to dentin among heat generated thermoplasticized gutta-percha technique. Bioinformation, 22(6), 3624-3628. https://doi.org/10.6026/973206300223624

Vancouver

Upadhayay A, Mishra P, Singh SK, Rajput S, Jain A, Sheikh K. Push-out bond strength of zinc oxide eugenol sealer, bioceramic sealer and bioactive glass sealer to dentin among heat generated thermoplasticized gutta-percha technique. Bioinformation. 2026;22(6):3624-3628. doi:10.6026/973206300223624

BibTeX
@article{Upadhayay2026,
  author = {Upadhayay, Ayushi and Mishra, Pankaj and Singh, Santosh Kumar and Rajput, Shubhashree and Jain, Ashee and Sheikh, Kehkashan},
  title = {Push-out bond strength of zinc oxide eugenol sealer, bioceramic sealer and bioactive glass sealer to dentin among heat generated thermoplasticized gutta-percha technique},
  journal = {Bioinformation},
  year = {2026},
  volume = {22},
  number = {6},
  pages = {3624--3628},
  doi = {10.6026/973206300223624}
}
Kostenlos starten →