Effects of Polyvinyl Alcohol – Hydroxyapatite Composite Ceramic on Calvarial Defects with Critical Size in Rat Models

Anu Dinesh, Francis B. Fernandez, Dinesh Parathazhathayil, Sooryadas Surendran, Pradep Mampilly, Anoop Sainulabdeen, N. S. Jinesh kumar, V. Remya, Varma Harikrishna

Journal of Lab Animal Research · 2024

DOI: 10.58803/jlar.v3i6.50 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Journal of Lab Animal Research, 2024. Verfasst von Anu Dinesh und 8 weiteren Autor:innen. Die Arbeit nennt 19 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0).

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Introduction

Biodegradable composite biomaterials are essential in healthcare, effectively tackling numerous complex challenges. Bone reconstruction is a surgical procedure aimed at remedying segmental bone loss, which is notably complicated and often fails to heal properly. A novel bone graft substitute incorporating polyvinyl alcohol (PVA) and synthetic hydroxyapatite (HA) has been developed and is tested in vivo in calvarial defect models of rat. The present study aimed to evaluate the bone regeneration potential of PVA – HA composite bone graft. Materials and methods: A total of 24 adult male Wistar rats aged 12-15 weeks with an average weight of 150 grams were used in the current study. A 4 mm full-thickness critical-size defect was created on the parietal bone and filled with the pre-sized graft material. Radiography, micro-computed tomography, scanning electron microscopy, histology, and serum biochemical parameters, including alkaline phosphatase and acid phosphatase activity, were utilized to evaluate the healing potential of the graft material. The animals were observed for twelve weeks. An immediate postoperative dorsoventral view of the skull was exposed at day zero and subsequent radiographs were taken periodically at weeks 2, 4, 8, and 12 in a group including 24 animals.

Results

Immediate post-operative radiographs revealed the radiolucent nature of the graft material. Throughout the healing process, it was observed that the graft remained in position and was intact. The values of serum biochemical parameters alkaline phosphatase and acid phosphatase activity) were haphazard throughout the observation period. In the 8th week, signs of progressive degradation of the graft material and bone regeneration could be seen, particularly on radiography, micro-CT scanning electron microscopy, and histologic examination.

Conclusion

It is concluded that the test graft material successfully accelerated bone regeneration and completely integrated with the host bone at week 12 of the experiment in the rat model.

Zitieren

APA

Dinesh, A., Fernandez, F. B., Parathazhathayil, D., Surendran, S., Mampilly, P., Sainulabdeen, A., kumar, N. S. J., Remya, V., & Harikrishna, V. (2024). Effects of Polyvinyl Alcohol – Hydroxyapatite Composite Ceramic on Calvarial Defects with Critical Size in Rat Models. Journal of Lab Animal Research. https://doi.org/10.58803/jlar.v3i6.50

Vancouver

Dinesh A, Fernandez FB, Parathazhathayil D, Surendran S, Mampilly P, Sainulabdeen A, et al. Effects of Polyvinyl Alcohol – Hydroxyapatite Composite Ceramic on Calvarial Defects with Critical Size in Rat Models. Journal of Lab Animal Research. 2024. doi:10.58803/jlar.v3i6.50

BibTeX
@article{Dinesh2024,
  author = {Dinesh, Anu and Fernandez, Francis B. and Parathazhathayil, Dinesh and Surendran, Sooryadas and Mampilly, Pradep and Sainulabdeen, Anoop and kumar, N. S. Jinesh and Remya, V. and Harikrishna, Varma},
  title = {Effects of Polyvinyl Alcohol – Hydroxyapatite Composite Ceramic on Calvarial Defects with Critical Size in Rat Models},
  journal = {Journal of Lab Animal Research},
  year = {2024},
  doi = {10.58803/jlar.v3i6.50}
}
Kostenlos starten →