EUVIMEDEUVIMED entdecken
Open Access · CC BY-SA 4.0

Enhanced Nickel Recovery from Mixed Hydroxide Precipitate Through Selective Leaching with KMnO4 Oxidant

Muhammad Dikdik Gumelar, Rahayu, Saputra, Agustanhakri, Husin, Andrameda, Taqwatomo, Putra, Indrijarso, Saudi, Indriasari, Arfiana und 3 weitere

Jurnal Sains Materi Indonesia · 06.08.2024 · 26 (1) · 35-44

DOI: 10.55981/jsmi.2024.3136 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Jurnal Sains Materi Indonesia, online erschienen am 06.08.2024. Verfasst von Muhammad Dikdik Gumelar und 14 weiteren Autor:innen. Die Arbeit wurde bisher 2-mal zitiert (Crossref) und nennt 27 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY-SA 4.0).

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Mixed Hydroxide Precipitate (MHP), a metal precipitate with the dominant nickel and cobalt content in hydroxide compounds, can be leached as a lithium battery precursor. In this study, KMnO4 was used as an oxidant agent to increase the solubility of Ni and Co. The variation of the sulfuric acid concentration (0.5 - 1.5 M) as a leachate reagent, the concentration of KMnO4 (2.5 - 7.5 g/L), and the selective leaching temperature (60 - 80°C) were investigated. Solvent extraction using CYANEX 272 and D2EHPA was performed to separate the Ni, Co, and Mn. Atomic Absorption Spectrometry (AAS), Inductively coupled plasma mass (ICP-OES), and X-ray Fluorescence (XRF) were used to analyze the chemical compositions. At the same time, crystallographic analysis was observed with X-Ray Diffraction. It was observed that potassium permanganate increased the dissolution of Ni and Co to 91.3% and 85.4% but decreased the dissolution of Mn (37.53%) under the following conditions: 1.75 M sulfuric acid, 7.5 g/L potassium permanganate, and 60°C temperature. High purity of nickel crystal (99.64%) was observed with spontaneous nucleation due to the supersaturated nickel solution after solvent extraction with CYANEX 272. Thus, using permanganate ion as selective leaching of Ni and Co from Mn is promising.

Zitieren

APA

Gumelar, M. D., Rahayu, Saputra, Agustanhakri, Husin, Andrameda, Taqwatomo, Putra, Indrijarso, Saudi, Indriasari, Arfiana, Yuliani, Mumtaz, & Mirahati (2024). Enhanced Nickel Recovery from Mixed Hydroxide Precipitate Through Selective Leaching with KMnO4 Oxidant. Jurnal Sains Materi Indonesia, 26(1), 35-44. https://doi.org/10.55981/jsmi.2024.3136

Vancouver

Gumelar MD, Rahayu, Saputra, Agustanhakri, Husin, Andrameda, et al. Enhanced Nickel Recovery from Mixed Hydroxide Precipitate Through Selective Leaching with KMnO4 Oxidant. Jurnal Sains Materi Indonesia. 2024;26(1):35-44. doi:10.55981/jsmi.2024.3136

BibTeX
@article{Gumelar2024,
  author = {Gumelar, Muhammad Dikdik and Rahayu and Saputra and Agustanhakri and Husin and Andrameda and Taqwatomo and Putra and Indrijarso and Saudi and Indriasari and Arfiana and Yuliani and Mumtaz and Mirahati},
  title = {Enhanced Nickel Recovery from Mixed Hydroxide Precipitate Through Selective Leaching with KMnO4 Oxidant},
  journal = {Jurnal Sains Materi Indonesia},
  year = {2024},
  volume = {26},
  number = {1},
  pages = {35--44},
  doi = {10.55981/jsmi.2024.3136}
}
Kostenlos starten →