EUVIMEDEUVIMED entdecken
Open Access

Effect of different design and surface treatment on the load-to- failure of ceramic repaired with composite

Mauricio Jm Tavares, Flavia Lb Amaral, Roberta T Basting, Cecilia P Turssi, Fabiana Mg França

Acta Odontológica Latinoamericana · 30.04.2024 · 37 (1) · 88-95

DOI: 10.54589/aol.37/1/88 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Acta Odontológica Latinoamericana, online erschienen am 30.04.2024. Verfasst von Mauricio Jm Tavares und 4 weiteren Autor:innen. Beteiligte Einrichtung: Faculdade Sao Leopoldo Mandíc, Instituto de Pesquisas Sao Leopoldo Mandic. Campinas/SP Brazil. Hauptthemen laut MEDLINE: Ceramics, Surface Properties, Dental Porcelain. Die Arbeit wurde bisher 4-mal zitiert (Crossref). Der Volltext ist frei in PubMed Central verfügbar.

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Glass ceramics are widely used to manufacture esthetic veneers, inlays, onlays, and crowns. Although the clinical survival rates of glass-ceramic restorations are favorable, fractures or chips are common. Certain cases can be repaired with direct composite.

Aim

The aim of this study was to investigate the interaction effect of different designs and surface treatments on the load-to-failure of lithium disilicate glass-ceramic repaired with nanofilled composite. Materials and Method: Lithium-disilicate glass-ceramic slabs (IPS e.max Press, Ivoclar Vivadent) with three different designs of the top surface (flat, single plateau, or double plateau) (n=11) received ‘no treatment’, ‘5% HF etching’, or “Al2O3 sandblasting”. HF-etched and sandblasted slabs also received silane and universal one-step adhesive application. All slabs were incrementally repaired with nanofilled composite (Filtek Z350, 3M ESPE) up to 6 mm above the highest ceramic top plateau. Specimens were stored in artificial saliva at 37 °C for 21 days and then subjected to 1,000 thermocycles between 5 and 55 °C. The interface composite-ceramic of each specimen was tensile tested until failure in a universal testing machine and the mode of failure was determined under a stereomicroscope. The ceramic surface morphology of one representative tested specimen from each subgroup (design/surface treatment) was observed through scanning electron microscopy (SEM).

Results

Regardless of ceramic design, the absence of surface treatment resulted in significantly lower load-to-failure values. No significant differences in load-to-failure values were observed between HF- etched and sandblasted specimens for the flat design; however, HF etching resulted in significantly higher load-to-failure values than sandblasting for both single plateau and double plateau designs. The majority (60%) of HF-etched specimens with single plateau or double plateau presented mixed failures. SEM photomicrographs showed that HF-etched specimens had smoother surfaces than sandblasted specimens.

Conclusion

The surface treatment of a defective lithium disilicate glass-ceramic restoration has more influence than its macroscopic design on the retention of the composite repair. HF etching seems to provide higher bond strength to the composite repair.

Schlagwörter

MeSH-Schlagwörter (MEDLINE)

CeramicsSurface PropertiesDental PorcelainMaterials TestingDental Restoration FailureComposite ResinsDental Stress AnalysisDental Prosthesis Design

Stichwörter der Autor:innen

ceramic repaircomposite repairdental restoration repairhydrofluoric acidsandblasting

Substanzen

Dental Porcelainlithia disilicateComposite Resins

Autor:innen und Institutionen

  • Faculdade Sao Leopoldo Mandíc, Instituto de Pesquisas Sao Leopoldo Mandic. Campinas/SP Brazil.
  • Faculdade Sao Leopoldo Mandíc, Instituto de Pesquisas Sao Leopoldo Mandic. Campinas/SP Brazil. biagomes@yahoo.com.

Zitieren

APA

Tavares, M. J., Amaral, F. L., Basting, R. T., Turssi, C. P., & França, F. M. (2024). Effect of different design and surface treatment on the load-to- failure of ceramic repaired with composite. Acta Odontológica Latinoamericana, 37(1), 88-95. https://doi.org/10.54589/aol.37/1/88

Vancouver

Tavares MJ, Amaral FL, Basting RT, Turssi CP, França FM. Effect of different design and surface treatment on the load-to- failure of ceramic repaired with composite. Acta Odontológica Latinoamericana. 2024;37(1):88-95. doi:10.54589/aol.37/1/88

BibTeX
@article{Tavares2024,
  author = {Tavares, Mauricio Jm and Amaral, Flavia Lb and Basting, Roberta T and Turssi, Cecilia P and França, Fabiana Mg},
  title = {Effect of different design and surface treatment on the load-to- failure of ceramic repaired with composite},
  journal = {Acta Odontológica Latinoamericana},
  year = {2024},
  volume = {37},
  number = {1},
  pages = {88--95},
  doi = {10.54589/aol.37/1/88}
}
Kostenlos starten →