EUVIMEDEUVIMED entdecken
Open Access · CC BY 4.0

Application of Rice Husk Ash-Derived Nano-Silica as a Partial Replacement of Portland Limestone Cement: Effects on Workability, Compressive Strength, and Mass Gain of Concrete

Adebola Saheed Akolade, Oluwatobiloba Dave Akintayo, Oluwatunmise Peter Abolarin, John Kehinde Adebayo, Precious Adesope Olaomotito, Abdulmoruf Olasile Akinsanya

American Journal of Civil Engineering and Constructions · 2026

DOI: 10.54536/ajcec.v2i2.8444 ↗

Kurz gefasst

Fachartikel in der Zeitschrift American Journal of Civil Engineering and Constructions, 2026. Verfasst von Adebola Saheed Akolade und 5 weiteren Autor:innen. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0).

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Rice husk ash (RHA) is a widely available agricultural waste with potential as a precursor for nano-silica, offering a supplementary cementitious material for concrete production. This study investigated the effect of nano-silica synthesised from RHA, calcined at 600 °C, as a partial replacement for Portland Limestone Cement (PLC) on the workability, compressive strength, and mass gain of concrete at 0%, 4%, and 8% replacement levels. The constituent fine and coarse aggregates were characterised for moisture content, specific gravity, and particle-size distribution before concrete production, and confirmed suitable for normal-weight concrete. Workability decreased progressively with increasing nano-silica content, with slump values dropping from 60 mm for the control mix to 45 mm and 35 mm at 4% and 8% replacement, respectively, although values remained within a workable range. The curing-period mass increase - measured here as the percentage increase in specimen mass between demoulding and the end of curing, and reported as a study-specific indicator distinct from standardised water absorption - was lowest at 4% replacement (0.66%), against 0.92% for the control and 0.71% at 8% replacement. The 8% replacement achieved the highest 28-day compressive strength, at 21.34 MPa, compared with 18.99 MPa at 4% replacement and 15.55 MPa for the control, associated with the combined filler, nucleation, and pozzolanic effects of nano-silica. Within the replacement levels investigated, 4% replacement provided the best overall balance of workability, compressive strength, and mass gain, while 8% replacement is better suited to applications where maximum 28-day compressive strength is the governing requirement. The findings demonstrate the potential of RHA-derived nano-silica as a supplementary cementitious material for PLC concrete, while providing a route for agricultural-waste valorization.

Zitieren

APA

Akolade, A. S., Akintayo, O. D., Abolarin, O. P., Adebayo, J. K., Olaomotito, P. A., & Akinsanya, A. O. (2026). Application of Rice Husk Ash-Derived Nano-Silica as a Partial Replacement of Portland Limestone Cement: Effects on Workability, Compressive Strength, and Mass Gain of Concrete. American Journal of Civil Engineering and Constructions. https://doi.org/10.54536/ajcec.v2i2.8444

Vancouver

Akolade AS, Akintayo OD, Abolarin OP, Adebayo JK, Olaomotito PA, Akinsanya AO. Application of Rice Husk Ash-Derived Nano-Silica as a Partial Replacement of Portland Limestone Cement: Effects on Workability, Compressive Strength, and Mass Gain of Concrete. American Journal of Civil Engineering and Constructions. 2026. doi:10.54536/ajcec.v2i2.8444

BibTeX
@article{Akolade2026,
  author = {Akolade, Adebola Saheed and Akintayo, Oluwatobiloba Dave and Abolarin, Oluwatunmise Peter and Adebayo, John Kehinde and Olaomotito, Precious Adesope and Akinsanya, Abdulmoruf Olasile},
  title = {Application of Rice Husk Ash-Derived Nano-Silica as a Partial Replacement of Portland Limestone Cement: Effects on Workability, Compressive Strength, and Mass Gain of Concrete},
  journal = {American Journal of Civil Engineering and Constructions},
  year = {2026},
  doi = {10.54536/ajcec.v2i2.8444}
}
Kostenlos starten →