Experimental Investigation of Composite Concrete by using Glass Powder as a Fine Aggregate and Ballast Stone as a Coarse Aggregate
International Journal of Advanced Research in Science Communication and Technology · 06.05.2026 · 98
DOI: 10.48175/ijarsct-34815 ↗Kurz gefasst
Fachartikel in der Zeitschrift International Journal of Advanced Research in Science Communication and Technology, online erschienen am 06.05.2026. Verfasst von Rahul Chandran R and Mrs. M. Priyanka. Die Arbeit nennt 15 Literaturangaben.
Abstract (Originalsprache)
Concrete is the mixture of various materials like coarse aggregate, fine aggregate, cement & water, each of them is mixed in various proportions to achieve specific strength. The fine and coarse aggregates are the main ingredients of concrete as the filler materials. As coarse aggregates are non renewable resources, scarcity of these materials have been increased in recent years. Therefore, it is essential to search for other materials, which can be used as an alternative to fine and coarse aggregate. Now days, waste of glasses are been increasing ,and the powder form of waste glass(GP) can be used as a partial replacement for the fine aggregates(FA), which can cause increase in the strength of concrete due to the proper alkali aggregate reaction up to 10% replacement. Brick ballast (BB) can be used as coarse aggregate partially in concrete. Cement being the most important material plays an important role in the manufacturing of concrete. The high cost of conventional construction materials is a dominating factor effecting constructions cost. This is necessity research for some new kind of alternative materials in the constructions field. Waste glass in the form of fine aggregate and brick ballast as coarse aggregate can be used. The proportion of the mineral and mixtures is applied in testing cubes for compression strength. This project briefly discusses the effects of addition of glass powder & brick ballast on the properties of mortar concrete mix of M25 at 14, and 28 days for concrete mix with brick ballast as 10%, 20%, 30%, 40%, & 50% of the weight coarse aggregate. Combination of these glass powder & brick ballast will gain the strength of nominal mix. Cubes of size 150x150x150 mm are constructed to check the compressive strength. The concrete made by the mixture glass powder & brick ballast is placed in the curing tank for 14 days and 28days for curing. The concrete is tested according to Indian standard specification to identify the compressive strength. This new technology will provide new solution for the disposal of glass sheet waste as well as the damaged or half burned bricks from the kiln
Zitieren
APA
Priyanka, R. C. R. A. M. M. (2026). Experimental Investigation of Composite Concrete by using Glass Powder as a Fine Aggregate and Ballast Stone as a Coarse Aggregate. International Journal of Advanced Research in Science Communication and Technology, 98. https://doi.org/10.48175/ijarsct-34815
Vancouver
Priyanka RCRAMM. Experimental Investigation of Composite Concrete by using Glass Powder as a Fine Aggregate and Ballast Stone as a Coarse Aggregate. International Journal of Advanced Research in Science Communication and Technology. 2026:98. doi:10.48175/ijarsct-34815
BibTeX
@article{Priyanka2026,
author = {Priyanka, Rahul Chandran R and Mrs. M.},
title = {Experimental Investigation of Composite Concrete by using Glass Powder as a Fine Aggregate and Ballast Stone as a Coarse Aggregate},
journal = {International Journal of Advanced Research in Science Communication and Technology},
year = {2026},
pages = {98},
doi = {10.48175/ijarsct-34815}
}
EUVIMED