EUVIMEDEUVIMED entdecken
Crossref

Deposition of Inconel 718 and Stellite 6 Coatings on Steel by Directed Energy Deposition and Evaluation of Cavitation Response under Ultrasonic Testing

Denis Andrei Predu, Ilare Bordeașu, Nicuşor Alin Sîrbu, Raluca Faur, Doru Alexandru Luca

Solid State Phenomena · 23.11.2026 · 396 · 25-36

DOI: 10.4028/p-z9fcc1 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Solid State Phenomena, online erschienen am 23.11.2026. Verfasst von Denis Andrei Predu und 4 weiteren Autor:innen. Die Arbeit nennt 15 Literaturangaben.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Two coatings deposited on steel by directed energy deposition (DED) were exposed to ultrasonic cavitation under a single laboratory protocol. The Inconel 718 coating was deposited on an InssTek MX-Mini system using a laser power of 230 W, a travel speed of 550 mm/min, a 0.15 mm layer height, a 0.30 mm step-over and a powder feed rate of 1.0 g/min; a second series was deposited by the same process route from Stellite 6, a cobalt-based Co-Cr-W-C hardfacing alloy. Both series used the same plain-carbon steel substrate and the same cylindrical specimen geometry. Cylindrical specimens were exposed in distilled water on a piezoceramic vibratory apparatus at a frequency of 20 ± 0.03 kHz, a vibration amplitude of 50 µm and a water temperature of 22 ± 1 °C, for a total attack time of 165 min. For the Stellite 6 series, cumulative mass loss was recorded gravimetrically at eight intermediate intervals and described by with A = 0.12, B = 3.873 × 10⁻³ and an endpoint cumulative mass loss of 9.35 mg. The Inconel 718 series was characterized after exposure by optical observation, scanning electron microscopy (SEM) and energy-dispersive X-ray spectroscopy (EDS). The eroded Inconel 718 surface showed a radial, flow-like morphology together with localized pits and shallow grooves, without macroscopic coating detachment in the examined fields. A representative EDS acquisition yielded 41.5 wt% Ni, 19.3 wt% Cr and 39.2 wt% Fe, normalized over three elements. The Ni-Cr signal confirms that the deposited layer was retained at the analyzed location, while the Fe level, more than twice the nominal content of Inconel 718, corresponds to a substrate dilution of the order of 20-25 % under a simple two-source mixing assumption. Deposition route, machine, substrate, specimen geometry and test conditions were common to the two series, although the Stellite 6 deposition ran under closed-loop laser-power control while the Inconel 718 parameters are reported at a fixed setting; the Stellite 6 data quantify the erosion kinetics of that common exposure, while the Inconel 718 data document damage morphology and near-surface chemistry. No quantitative resistance ranking between the two coatings is claimed, because gravimetric records were acquired only for the Stellite 6 series.

Zitieren

APA

Predu, D. A., Bordeașu, I., Sîrbu, N. A., Faur, R., & Luca, D. A. (2026). Deposition of Inconel 718 and Stellite 6 Coatings on Steel by Directed Energy Deposition and Evaluation of Cavitation Response under Ultrasonic Testing. Solid State Phenomena, 396, 25-36. https://doi.org/10.4028/p-z9fcc1

Vancouver

Predu DA, Bordeașu I, Sîrbu NA, Faur R, Luca DA. Deposition of Inconel 718 and Stellite 6 Coatings on Steel by Directed Energy Deposition and Evaluation of Cavitation Response under Ultrasonic Testing. Solid State Phenomena. 2026;396:25-36. doi:10.4028/p-z9fcc1

BibTeX
@article{Predu2026,
  author = {Predu, Denis Andrei and Bordeașu, Ilare and Sîrbu, Nicuşor Alin and Faur, Raluca and Luca, Doru Alexandru},
  title = {Deposition of Inconel 718 and Stellite 6 Coatings on Steel by Directed Energy Deposition and Evaluation of Cavitation Response under Ultrasonic Testing},
  journal = {Solid State Phenomena},
  year = {2026},
  volume = {396},
  pages = {25--36},
  doi = {10.4028/p-z9fcc1}
}
Kostenlos starten →