EUVIMEDEUVIMED entdecken
Crossref

Fretting Fatigue and Crack Initiation Analysis of 42CrMo4+QT and 34CrNiMo6+QT Steels

Martin Nesládek, Marius Müller, Vladimír Mára, Tomáš Karas, Jan Papuga, Alexander Hasse

Key Engineering Materials · 05.12.2025 · 1035 · 71-83

DOI: 10.4028/p-0dsktu ↗

Kurz gefasst

Fachartikel in der Zeitschrift Key Engineering Materials, online erschienen am 05.12.2025. Verfasst von Martin Nesládek und 5 weiteren Autor:innen. Die Arbeit wurde bisher 1-mal zitiert (Crossref) und nennt 20 Literaturangaben.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Reliable fretting fatigue prediction requires rigorous evaluation of analytical methods under realistic loading conditions. This study builds upon previous research on the fretting fatigue behavior of 42CrMo4+QT steel by incorporating new experimental data from square cross-section specimens tested under axial loading with various pad geometries. The application of a non-zero tensile mean bulk load promoted localized crack initiation near the specimen edges, leading to more asymmetric crack growth in the majority of cases unlike the more symmetric behavior observed under fully reversed loading (R = –1). Finite element analysis (FEA), along with the Dang Van and Papuga QCP methods, was employed to evaluate whether this behavior could be accurately modeled. In addition, a linear-elastic fracture mechanics approach was used to model and explain these observations. Furthermore, fretting fatigue tests on 34CrNiMo6+QT steel revealed that tribological effects governed crack initiation, in contrast to the stress-driven failure observed in 42CrMo4+QT. These findings enhance understanding of fretting fatigue mechanisms and improve predictive modeling approaches.

Zitieren

APA

Nesládek, M., Müller, M., Mára, V., Karas, T., Papuga, J., & Hasse, A. (2025). Fretting Fatigue and Crack Initiation Analysis of 42CrMo4+QT and 34CrNiMo6+QT Steels. Key Engineering Materials, 1035, 71-83. https://doi.org/10.4028/p-0dsktu

Vancouver

Nesládek M, Müller M, Mára V, Karas T, Papuga J, Hasse A. Fretting Fatigue and Crack Initiation Analysis of 42CrMo4+QT and 34CrNiMo6+QT Steels. Key Engineering Materials. 2025;1035:71-83. doi:10.4028/p-0dsktu

BibTeX
@article{Nesldek2025,
  author = {Nesládek, Martin and Müller, Marius and Mára, Vladimír and Karas, Tomáš and Papuga, Jan and Hasse, Alexander},
  title = {Fretting Fatigue and Crack Initiation Analysis of 42CrMo4+QT and 34CrNiMo6+QT Steels},
  journal = {Key Engineering Materials},
  year = {2025},
  volume = {1035},
  pages = {71--83},
  doi = {10.4028/p-0dsktu}
}
Kostenlos starten →