A New Assessment of Multilayer Ceramic Capacitor Crack Severity
Pan Pacific Symposium · 2026-02 · 29 (1) · 155-160
DOI: 10.37665/ppeqrgo70395 ↗Kurz gefasst
Fachartikel in der Zeitschrift Pan Pacific Symposium, 2026-02. Verfasst von Theron Lewis und 6 weiteren Autor:innen.
Abstract (Originalsprache)
Multilayer Ceramic Capacitors (MLCCs) are among the most widely utilized passive components in surface-mount technology (SMT) for modern electronic systems. These capacitors are constructed by stacking alternating layers of ceramic dielectric and metal electrodes, which are then sintered and terminated to form a compact, high-capacitance device. MLCCs are valued for their small footprint, broad capacitance range—from picofarads to microfarads—and voltage ratings that span from a few volts to several hundred volts. Despite their widespread use and reliability, MLCCs are inherently susceptible to mechanical and environmental stress due to their ceramic composition, which can lead to cracking within the body of the component. Cracks in MLCCs are a significant reliability concern, especially because they are often not detectable with standard inspection methods. These fractures typically originate from mechanical stress during printed circuit board (PCB) assembly, particularly when MLCCs are placed near board edges or subjected to flexing during depaneling. Additional contributors include thermal stress from soldering processes, improper mounting techniques, and environmental factors such as vibration and shock. Once a crack forms, it can lead to a range of failure modes including open circuits, parametric drift, reduced insulation resistance, intermittent electrical behavior, and corrosion or electrochemical migration. The most severe consequence is a short circuit failure, which can result in localized heating, component burnout, and potential damage to surrounding circuitry. The unpredictability of crack-related failures poses a challenge for reliability assessments. Not all cracks result in catastrophic shorts; some may only cause minor electrical deviations or remain dormant. This project investigates the correlation between application stress levels and the likelihood of severe MLCC failures. Specifically, it demonstrates that MLCCs operating in low-stress environments are less prone to short circuit failures compared to those in high-stress conditions. Furthermore, the study explores how the severity of the crack and ambient humidity levels influence the probability of a short occurring. Higher humidity can accelerate degradation through moisture ingress, increasing the risk of electrical bridging across fractured dielectric layers. To enhance failure analysis capabilities, this work also incorporates magnetic field imaging techniques to visualize current paths and identify fault locations within cracked MLCCs. Using advanced magnetic microscopy, such as SQUID, the internal structure and electrical behavior of damaged capacitors can be examined non-destructively. This imaging reveals how severe cracks manifest under magnetic field analysis and provides insight into the internal failure mechanisms that are otherwise hidden from view. In summary, this research highlights the critical role of mechanical integrity, environmental conditions, and advanced diagnostic tools in understanding and mitigating MLCC failures.
Zitieren
APA
Lewis, T., Bielick, J., Czarnecki, J., Lei, C. C., Leung, T., Shevach, S., & Wassick, T. (2026). A New Assessment of Multilayer Ceramic Capacitor Crack Severity. Pan Pacific Symposium, 29(1), 155-160. https://doi.org/10.37665/ppeqrgo70395
Vancouver
Lewis T, Bielick J, Czarnecki J, Lei CC, Leung T, Shevach S, et al. A New Assessment of Multilayer Ceramic Capacitor Crack Severity. Pan Pacific Symposium. 2026;29(1):155-160. doi:10.37665/ppeqrgo70395
BibTeX
@article{Lewis2026,
author = {Lewis, Theron and Bielick, Jim and Czarnecki, John and Lei, Chon C and Leung, Tak and Shevach, Steven and Wassick, Tom},
title = {A New Assessment of Multilayer Ceramic Capacitor Crack Severity},
journal = {Pan Pacific Symposium},
year = {2026},
volume = {29},
number = {1},
pages = {155--160},
doi = {10.37665/ppeqrgo70395}
}