Dimensional Stability of Ambient-Cured One-Part Geopolymer Concrete Activated by Powdered Sodium Metasilicate: Drying Shrinkage, Restrained Shrinkage and Creep

Allanazar Ilyasov, Azamat Nazibekov

The American Journal of Engineering and Technology · 01.06.2026 · 8 (6) · 207-213

DOI: 10.37547/tajet/volume08issue06-18 ↗

Kurz gefasst

Fachartikel in der Zeitschrift The American Journal of Engineering and Technology, online erschienen am 01.06.2026. Verfasst von Allanazar Ilyasov und 1 weiteren Autor:innen.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Dimensional stability is one of the key serviceability criteria for geopolymer concrete, especially when the binder is produced by a one-part route and cured at ambient temperature. This paper evaluates drying shrinkage, restrained shrinkage and compressive creep of one-part geopolymer concrete activated mainly with powdered sodium metasilicate anhydrous. The binder system was based on class F fly ash and ground granulated blast furnace slag (GGBFS), and the assessment focused on the effects of slag content, water-to-precursor ratio and solid activator composition. Five one-part mixtures were compared with an ordinary Portland cement concrete reference. Free shrinkage was monitored for one year together with mass loss and ultrasonic pulse velocity, while restrained shrinkage was measured on slab specimens by a photogrammetry-based procedure. Creep was evaluated under sustained compressive stress applied at 28 days. The slag-dominant mixture showed the highest one-year free shrinkage, reaching 1769 microstrain, whereas mixtures containing 60% fly ash and 40% GGBFS generally remained between 723 and 1091 microstrain. Lowering the water-to-precursor ratio from 0.45 to 0.35 reduced creep strain from about 1706 to 1551 microstrain and decreased the creep coefficient from 2.56 to 1.87. Restrained shrinkage of geopolymer mixtures was markedly lower than that of the Portland cement reference, with optimized mixtures remaining around 255-270 microstrain after one year. The results show that powdered sodium metasilicate can produce dimensionally stable one-part geopolymer concrete when slag content and water dosage are controlled to limit mesopore development, capillary pressure and early-age self-desiccation.

Zitieren

APA

Ilyasov, A., & Nazibekov, A. (2026). Dimensional Stability of Ambient-Cured One-Part Geopolymer Concrete Activated by Powdered Sodium Metasilicate: Drying Shrinkage, Restrained Shrinkage and Creep. The American Journal of Engineering and Technology, 8(6), 207-213. https://doi.org/10.37547/tajet/volume08issue06-18

Vancouver

Ilyasov A, Nazibekov A. Dimensional Stability of Ambient-Cured One-Part Geopolymer Concrete Activated by Powdered Sodium Metasilicate: Drying Shrinkage, Restrained Shrinkage and Creep. The American Journal of Engineering and Technology. 2026;8(6):207-213. doi:10.37547/tajet/volume08issue06-18

BibTeX
@article{Ilyasov2026,
  author = {Ilyasov, Allanazar and Nazibekov, Azamat},
  title = {Dimensional Stability of Ambient-Cured One-Part Geopolymer Concrete Activated by Powdered Sodium Metasilicate: Drying Shrinkage, Restrained Shrinkage and Creep},
  journal = {The American Journal of Engineering and Technology},
  year = {2026},
  volume = {8},
  number = {6},
  pages = {207--213},
  doi = {10.37547/tajet/volume08issue06-18}
}
Kostenlos starten →