Fachartikel in der Zeitschrift International Journal of Applied Sciences & Development, online erschienen am 19.11.2026. Verfasst von Delia Teresa Sponza und 1 weiteren Autor:innen. Die Arbeit nennt 59 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0).

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

A high density polyethylene (HDPE) plastic was reused and it was used together with cerium dioxide (CeO2) to photodegrade the Roxarsone (ROX, 4-hydroxy-3-nitrophenylarsonic acid). The microstructure of the HPDE/CeO2 polymer nanocomposite was characterized by scanning electron microscopy (SEM) analysis, energy In the sunlight power (20-100 W/m2), photooxidation time (10 – 100 min), pH (2-10), temperature (10oC-40oC), HDPE nanocomposites (NCs) concentrations (100-1600 mg/l), CeO2 concentrations (2.5-18 mg/l) and the ratios of HDPE to CeO2 (37.5-100), HDPE/CeO2 NCs concentration (200-2400 mg/l) on the photodegradation yields of ROX was investigated. The surface properties of the HDPE/CeO2 NCs was investigated by the XRD, SEM and FTIR analysis. For maximum photodegradation yields of ROX (99%) the optimum operational conditions were 60 W/m2 sunlight power, pH=4.0, 40oC, at 8 mg/l CeO2 nanoparticles (NPs), at 300 mg/l HDPE concentration, at a HDPE TO CeO2 ratio of 37.5, at 800 mg/l ROX concentration, after 30 min photodegradation duration, respectively. ROX was photodegraded according to Hinshelwood Kinetic with a reaction kinetic constant of k = 12.349 x 10-4 min-1. EDS analysis showed that Ce and O were distributed on the surface and CeO2 particles existed in the HDPE matrix. According to SEM analyses the aging treatment increased the adhesive wear level on the HDPE/CeO2 NCs by leading to the increase of coefficients of friction (COF). XRD results showed that the characteristic peaks of the HDPE without aging were higher, and the height of the characteristic peak decreased after aging treatment. Therefore, the crystallinity of HDPE decreased, and showed that the fracture of internal molecular chain increased after aging treatment.

Zitieren

APA

Sponza, D. T., & Öztekin, R. (2026). The Reuse of High-Density Polyethylene (HDPE) Plastic Wastes and their Usage with Cerium Dioxide (CeO2) as New Polymer Nanocomposites. International Journal of Applied Sciences & Development, 5, 220. https://doi.org/10.37394/232029.2026.5.23

Vancouver

Sponza DT, Öztekin R. The Reuse of High-Density Polyethylene (HDPE) Plastic Wastes and their Usage with Cerium Dioxide (CeO2) as New Polymer Nanocomposites. International Journal of Applied Sciences & Development. 2026;5:220. doi:10.37394/232029.2026.5.23

BibTeX
@article{Sponza2026,
  author = {Sponza, Delia Teresa and Öztekin, Rukiye},
  title = {The Reuse of High-Density Polyethylene (HDPE) Plastic Wastes and their Usage with Cerium Dioxide (CeO2) as New Polymer Nanocomposites},
  journal = {International Journal of Applied Sciences & Development},
  year = {2026},
  volume = {5},
  pages = {220},
  doi = {10.37394/232029.2026.5.23}
}
Kostenlos starten →