Silver leaching from wasted printed circuit boards using choline chloride-based ternary deep eutectic solvents

Soja Siti Fatimah, Yosefani Anastasiya Simanungkalit, Muhammad Riyu Chieka, Jaaka Yarfa Alhaqqa, Omay Sumarna, Abraham Mora

Physicochemical Problems of Mineral Processing · 10.03.2026

DOI: 10.37190/ppmp/219012 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Physicochemical Problems of Mineral Processing, online erschienen am 10.03.2026. Verfasst von Soja Siti Fatimah und 5 weiteren Autor:innen. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0).

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

In this study, we developed two TDES systems- choline chloride (ChCl)-glycerol (Gly)-malic acid (MA), labelled as TDES 1, and ChCl-ethylene glycol (EG)-citric acid (CA), as TDES 2, for silver leaching from wasted printed circuit boards (WPCBs). Viscosity, density, pH, and solubility measurements were conducted to observe the physical characteristics of TDES. Both TDES systems were polar and exhibited a pH of 2. Increasing the molar ratio of the hydrogen-bond acceptor (HBA) decreased the viscosity of the TDES, whereas increasing the molar ratio of the hydrogen-bond donor (HBD) increased the viscosity of the DES. Fourier-transform infrared spectroscopy (FTIR) analysis revealed hydrogen-bond interactions between components in TDES, indicated by shifts in the functional group wavenumbers. Differential scanning calorimetry (DSC) showed thermal transitions, including partial melting, cold crystallization, and secondary phase changes, confirming the formation of stable eutectic systems. TDES 1 (1:2:1 molar ratio) and TDES 2 (2:1:1 molar ratio) were used as lixiviants to extract silver from WPCBs. The optimum leaching temperature for both TDES was 120 °C, with a solid-to-liquid (S/L) ratio of 1/100. The optimum leaching duration was 6 h for TDES 1 and 9 h for TDES 2. Under optimum conditions, TDES 1 and TDES 2 achieved efficiencies of 98.36% and 94.82%, respectively, highlighting their effectiveness in recovering silver from PCB waste. Both TDES offer potential as efficient and environmentally sustainable solvents for the recovery of critical metals from electronic components. This approach supports better resource recovery and a circular economy for electronic waste management.

Zitieren

APA

Fatimah, S. S., Simanungkalit, Y. A., Chieka, M. R., Alhaqqa, J. Y., Sumarna, O., & Mora, A. (2026). Silver leaching from wasted printed circuit boards using choline chloride-based ternary deep eutectic solvents. Physicochemical Problems of Mineral Processing. https://doi.org/10.37190/ppmp/219012

Vancouver

Fatimah SS, Simanungkalit YA, Chieka MR, Alhaqqa JY, Sumarna O, Mora A. Silver leaching from wasted printed circuit boards using choline chloride-based ternary deep eutectic solvents. Physicochemical Problems of Mineral Processing. 2026. doi:10.37190/ppmp/219012

BibTeX
@article{Fatimah2026,
  author = {Fatimah, Soja Siti and Simanungkalit, Yosefani Anastasiya and Chieka, Muhammad Riyu and Alhaqqa, Jaaka Yarfa and Sumarna, Omay and Mora, Abraham},
  title = {Silver leaching from wasted printed circuit boards using choline chloride-based ternary deep eutectic solvents},
  journal = {Physicochemical Problems of Mineral Processing},
  year = {2026},
  doi = {10.37190/ppmp/219012}
}
Kostenlos starten →