Effect of steady magnetic field on microstructure and microhardness of laser-directed energy-deposited Ti6Al4V/TiC composite coatings
Materials Science in Additive Manufacturing · 16.11.2026 · 026360090
DOI: 10.36922/msam026360090 ↗Kurz gefasst
Fachartikel in der Zeitschrift Materials Science in Additive Manufacturing, online erschienen am 16.11.2026. Verfasst von Qingmei Qian und 2 weiteren Autor:innen.
Abstract (Originalsprache)
Coarse microstructures, reinforcement agglomeration, and non-uniform property distribution are critical issues in laser-directed energy-deposited Ti6Al4V/TiC composite coatings. To address these issues, this study adopts a steady magnetic field with gradient intensities to assist the laser-directed energy deposition process. Ti-based composite coatings were fabricated on Ti6Al4V substrates under three laser processes with different heat inputs. Macroscopic observation, microstructural characterization, and microhardness tests were performed to investigate the coupled effects of magnetic field strength and laser heat input on coating formation quality, microstructural evolution, and microhardness. A magnetic modulation coupling coefficient K was proposed to quantitatively evaluate the modulation performance. The results show that the steady magnetic field effectively improved the macroscopic forming quality of the coatings. Surface defects decreased, and the wetting angle increased monotonically with rising magnetic field strength. The magnetic field’s modulation of microstructure and hardness was highly process-dependent. Under medium- (1,000 W, 350 mm/min, 1.2 r/min) and low-heat-input processes (800 W, 350 mm/min, 1.0 r/min), a low magnetic field of 4.07 mT yielded the optimal grain refinement and TiC dispersion uniformity. For the low-heat-input process, coating hardness first decreased slightly and then increased continuously with increasing magnetic field strength. For the medium-heat-input process, hardness increased monotonically, reaching its maximum at 12.11 mT. Under the high-heat-input process (1,200 W, 250 mm/min, 1.0 r/min), a low magnetic field aggravated microstructural coarsening, and significant strengthening was achieved only when the field strength reached 12.11 mT. The maximum coating hardness reached 1155.16 HV0.2, 50.85% higher than that of the sample without a magnetic field. The hardness evolution is governed by the combined effect of grain refinement and second-phase evolution. The proposed coupling coefficient can effectively quantify the interaction between the magnetic field and laser energy, providing a theoretical reference for optimizing steady-magnetic-field-assisted laser-directed energy deposition.
Zitieren
APA
Qian, Q., Yang, Q., & Zeng, C. (2026). Effect of steady magnetic field on microstructure and microhardness of laser-directed energy-deposited Ti6Al4V/TiC composite coatings. Materials Science in Additive Manufacturing, 0(0), 026360090. https://doi.org/10.36922/msam026360090
Vancouver
Qian Q, Yang Q, Zeng C. Effect of steady magnetic field on microstructure and microhardness of laser-directed energy-deposited Ti6Al4V/TiC composite coatings. Materials Science in Additive Manufacturing. 2026;0(0):026360090. doi:10.36922/msam026360090
BibTeX
@article{Qian2026,
author = {Qian, Qingmei and Yang, Quanou and Zeng, Chao},
title = {Effect of steady magnetic field on microstructure and microhardness of laser-directed energy-deposited Ti6Al4V/TiC composite coatings},
journal = {Materials Science in Additive Manufacturing},
year = {2026},
volume = {0},
number = {0},
pages = {026360090},
doi = {10.36922/msam026360090}
}