EUVIMEDEUVIMED entdecken
Open Access · CC BY 4.0

Optimization of Gear Sprocket Surface Hardness through a Combination of Ice Water Quenching and Shot Peening with Pressure Variations

Bambang Hari Priyambodo, Widia Setiawan, Handoko, Martinus Heru Palmiyanto Palmiyanto, Kaleb Priyanto, Yani Kurniawan

Teknobiz : Jurnal Ilmiah Program Studi Magister Teknik Mesin · 04.03.2026 · 16 (1) · 70-76

DOI: 10.35814/nttrpa77 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Teknobiz : Jurnal Ilmiah Program Studi Magister Teknik Mesin, online erschienen am 04.03.2026. Verfasst von Bambang Hari Priyambodo und 5 weiteren Autor:innen. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0).

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

The gear sprocket is a transmission system component that operates under repeated torsional and frictional loads, making its surface susceptible to wear. To improve wear resistance, a treatment is required to harden the surface layer without significantly altering its dimensions. This study aims to evaluate the effect of combining ice-water quenching and varying shot peening pressures on the surface hardness and microstructural changes of a medium carbon steel gear sprocket. The specimens were austenitized at 850 °C for 15 minutes and rapidly cooled using ice water. Subsequent shot peening was performed for 20 minutes using 0.6 mm diameter steel shots at pressures of 5, 6, 7, and 8 bar. Surface hardness was measured using the Vickers (HV) method, and microstructural observations were conducted with an optical microscope after 2% Nital etching to identify phase transformations. The results show that ice-water quenching increased the surface hardness from 199 HV to 329 HV, representing an increase of approximately 65% over the untreated condition. The combination of quenching and shot peening further enhanced hardness to 404 HV, 454 HV, 487 HV, and 552 HV at 5, 6, 7, and 8 bar, respectively, with the maximum improvement reaching 177% compared to the untreated specimen. Microstructural analysis revealed fine martensitic structures on the quenched surface and a plastically deformed layer produced by shot impacts. Therefore, the combination of ice-water quenching and shot peening effectively enhances surface hardness and refines the microstructure of gear sprockets, indicating its potential application in improving the transmission components wear resistance.

Zitieren

APA

Priyambodo, B. H., Setiawan, W., Handoko, Palmiyanto, M. H. P., Priyanto, K., & Kurniawan, Y. (2026). Optimization of Gear Sprocket Surface Hardness through a Combination of Ice Water Quenching and Shot Peening with Pressure Variations. Teknobiz : Jurnal Ilmiah Program Studi Magister Teknik Mesin, 16(1), 70-76. https://doi.org/10.35814/nttrpa77

Vancouver

Priyambodo BH, Setiawan W, Handoko, Palmiyanto MHP, Priyanto K, Kurniawan Y. Optimization of Gear Sprocket Surface Hardness through a Combination of Ice Water Quenching and Shot Peening with Pressure Variations. Teknobiz : Jurnal Ilmiah Program Studi Magister Teknik Mesin. 2026;16(1):70-76. doi:10.35814/nttrpa77

BibTeX
@article{Priyambodo2026,
  author = {Priyambodo, Bambang Hari and Setiawan, Widia and Handoko and Palmiyanto, Martinus Heru Palmiyanto and Priyanto, Kaleb and Kurniawan, Yani},
  title = {Optimization of Gear Sprocket Surface Hardness through a Combination of Ice Water Quenching and Shot Peening with Pressure Variations},
  journal = {Teknobiz : Jurnal Ilmiah Program Studi Magister Teknik Mesin},
  year = {2026},
  volume = {16},
  number = {1},
  pages = {70--76},
  doi = {10.35814/nttrpa77}
}
Kostenlos starten →