The effect of using 40% HF treatment on the shear bond strength of the zirconia surface in comparison to conventional surface treatment methods
Journal of Lasers in Medical Sciences · 30.05.2026 · 17 · e48130
DOI: 10.34172/jlms.48130 ↗Kurz gefasst
Fachartikel in der Zeitschrift Journal of Lasers in Medical Sciences, online erschienen am 30.05.2026. Verfasst von Rahab Ghoveizi und 4 weiteren Autor:innen. Beteiligte Einrichtung: Department of Prosthodontics, School of Dentistry, Shahid Beheshti University of Medical Sciences, Tehran, Iran. Die Arbeit nennt 43 Literaturangaben. Der Volltext ist frei in PubMed Central verfügbar.
Abstract (Originalsprache)
Introduction
The goal of this investigation was to examine how various surface preparation techniques affect the Shear Bond Strength (SBS) of resin cement to zirconia restorations.
Methods
120 samples of zirconia ceramic disks in eight categories (10 x 3 mm) were randomly selected: 1. Control group (no surface treatments), 2. AL₂O₃ particle sandblasting, 3. 2.5 W Nd/YAG laser, 4. 3 W Nd/YAG laser, 5. Sandblasting plus 2.5 W Nd/YAG laser, 6. Sandblasting plus 3 W Nd/YAG laser, 7. 40% Hydrofluoric acid (HF), and 8. Sandblasting plus 40% HF. The analysis of one sample from each group was done using scanning. PANAVIA F2 dual-cure resin cement was then used to attach the samples to the composite resin. After thermocycling, the present researchers conducted the shear bond strength test utilizing the universal testing machine. The data were statistically evaluated using the Welch and Games-Howell tests, with a significance threshold of 0.05.
Results
A statistically significant difference (P0.05). Sandblasting with HF acid etching had the greatest SBS, measuring 13.04 MPa. Out of all the groups, the SBS value was lowest for the control group (3.85 MPa). In terms of fracture type, the control group experienced more adhesive fractures. In the sandblasting and 3 W laser groups, the mixed and adhesive fractures were equal, and the mixed fracture was the most common type in the other groups.
Conclusion
The greatest SBS was obtained by sandblasting combined with etching. Nevertheless, this disparity was not statistically significant. In all groups but the control group, the SBS was not statistically significant.
Schlagwörter
Stichwörter der Autor:innen
Autor:innen und Institutionen
- Department of Prosthodontics, School of Dentistry, Shahid Beheshti University of Medical Sciences, Tehran, Iran.
ORCID-Profile: Rahab Ghoveizi, Pejman Moradi
Zitieren
APA
Ghoveizi, R., Beyabanaki, E., Tavakolizadeh, S., Samadnezhad, A., & Moradi, P. (2026). The effect of using 40% HF treatment on the shear bond strength of the zirconia surface in comparison to conventional surface treatment methods. Journal of Lasers in Medical Sciences, 17, e48130. https://doi.org/10.34172/jlms.48130
Vancouver
Ghoveizi R, Beyabanaki E, Tavakolizadeh S, Samadnezhad A, Moradi P. The effect of using 40% HF treatment on the shear bond strength of the zirconia surface in comparison to conventional surface treatment methods. Journal of Lasers in Medical Sciences. 2026;17:e48130. doi:10.34172/jlms.48130
BibTeX
@article{Ghoveizi2026,
author = {Ghoveizi, Rahab and Beyabanaki, Elaheh and Tavakolizadeh, Sara and Samadnezhad, Aynaz and Moradi, Pejman},
title = {The effect of using 40% HF treatment on the shear bond strength of the zirconia surface in comparison to conventional surface treatment methods},
journal = {Journal of Lasers in Medical Sciences},
year = {2026},
volume = {17},
pages = {e48130},
doi = {10.34172/jlms.48130}
}
EUVIMED