Fachartikel in der Zeitschrift Sci, online erschienen am 30.05.2026. Verfasst von Umanath R. Poojary und 2 weiteren Autor:innen. Die Arbeit nennt 42 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0).
Abstract (Originalsprache)
Mechanical components subjected to dynamic loading require materials that combine adequate strength with effective vibration-damping capability. Austempered ductile iron (ADI) is a promising candidate for such applications because of its ausferritic matrix, which provides a useful combination of strength, toughness, wear resistance, and energy dissipation. However, the damping behaviour of manganese-alloyed ADI and its dependence on austempering parameters have not been sufficiently clarified. In this study, ductile iron containing 0.3, 0.6, and 0.9 wt% Mn was austempered at 320, 370, and 420 °C for 1, 1.5, and 2 h using a full-factorial experimental design. The damping response was evaluated through impact hammer-based experimental modal analysis and correlated with hardness, ausferritic morphology, and the volume fraction of carbon-enriched/high-carbon austenite. The results showed that manganese content and austempering temperature significantly influenced the loss factor, whereas austempering time had only a minor effect within the selected range. The highest damping performance was obtained for the alloy containing 0.6 wt% Mn austempered at 370 °C, where a favourable balance was achieved between stabilized high-carbon austenite, refined ausferritic morphology, ferrite/austenite interface density, and controlled matrix hardness. At 320 °C, limited austenite stabilization restricted damping improvement, while at 420 °C, ausferritic coarsening reduced the effective interface-related energy dissipation. ANOVA confirmed manganese content and austempering temperature as the dominant factors, contributing approximately 59% and 39%, respectively, to the variation in loss factor. The regression model showed strong predictive capability within the investigated process window. Overall, the study demonstrates that damping behaviour in manganese-alloyed ADI can be effectively tailored through controlled alloy chemistry and austempering temperature, supporting its potential use in vibration-sensitive engineering components.
Zitieren
APA
Poojary, U. R., Hegde, A., & Hegde, S. (2026). Data-Driven Modelling of Damping Behaviour in Austempered Ductile Iron: Influence of Manganese Content and Heat Treatment Parameters. Sci, 8(6), 128. https://doi.org/10.3390/sci8060128
Vancouver
Poojary UR, Hegde A, Hegde S. Data-Driven Modelling of Damping Behaviour in Austempered Ductile Iron: Influence of Manganese Content and Heat Treatment Parameters. Sci. 2026;8(6):128. doi:10.3390/sci8060128
BibTeX
@article{Poojary2026,
author = {Poojary, Umanath R. and Hegde, Ananda and Hegde, Sriharsha},
title = {Data-Driven Modelling of Damping Behaviour in Austempered Ductile Iron: Influence of Manganese Content and Heat Treatment Parameters},
journal = {Sci},
year = {2026},
volume = {8},
number = {6},
pages = {128},
doi = {10.3390/sci8060128}
}
EUVIMED