EUVIMEDEUVIMED entdecken
Open Access · CC BY 4.0

Recovery of Valuable Metals from Spent Lithium-Ion Batteries by Combining Reduction Roasting and Selective Leaching

Ruijiao Zhai, Kui Huang, Shanjin Mao, Rugui Li, Haili Dong, Xi Zhai

Recycling · 10.03.2026 · 11 (3) · 59

DOI: 10.3390/recycling11030059 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Recycling, online erschienen am 10.03.2026. Verfasst von Ruijiao Zhai und 5 weiteren Autor:innen. Die Arbeit wurde bisher 2-mal zitiert (Crossref) und nennt 55 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: National Natural Science Foundation of China, Guangxi Scientific and Technology Plan Project, Scientific Research Foundation of Guangxi University.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Amid growing environmental pressure and increasing demand for resource sustainability, the efficient recovery of valuable metals from spent lithium-ion batteries (LIBs) has become a critical challenge in the field of resource recycling. Therefore, a novel approach is presented for selective lithium (Li) and manganese (Mn) separation from LiNixCoyMn1−x−yO2 by combining carbothermic reduction roasting and selective leaching. Low-cost glucose (C6H12O6) was selected as the reduction roasting reductant, which converts the cathode materials into water-soluble lithium carbonate (Li2CO3), water-insoluble cobalt (Co), nickel (Ni), and manganese oxide (MnO). Wet magnetic separation was employed to preferentially extract Li while simultaneously removing excess carbon from Ni, Co, and MnO. Under optimal roasting conditions at 600 °C for 90 min followed by wet magnetic separation with a liquid–solid ratio of 30 mL/g for 30 min, 95.42% of Li was preferentially extracted. Subsequently, at a formic acid (HCOOH) concentration of 1.6 mol/L, liquid–solid ratio of 6 mL/g, and leaching time of 30 min, 94.29% of Mn was selectively extracted from the wet magnetic separation products, whereas Ni and Co were leached at 6.13% and 7.22%, respectively. The acid-leaching residue can be recycled as a Ni-Co alloy.

Förderung

  • National Natural Science Foundation of China
  • Guangxi Scientific and Technology Plan Project
  • Scientific Research Foundation of Guangxi University
  • Guangxi Bossco Environmental Protection Technology Co., Ltd.

Zitieren

APA

Zhai, R., Huang, K., Mao, S., Li, R., Dong, H., & Zhai, X. (2026). Recovery of Valuable Metals from Spent Lithium-Ion Batteries by Combining Reduction Roasting and Selective Leaching. Recycling, 11(3), 59. https://doi.org/10.3390/recycling11030059

Vancouver

Zhai R, Huang K, Mao S, Li R, Dong H, Zhai X. Recovery of Valuable Metals from Spent Lithium-Ion Batteries by Combining Reduction Roasting and Selective Leaching. Recycling. 2026;11(3):59. doi:10.3390/recycling11030059

BibTeX
@article{Zhai2026,
  author = {Zhai, Ruijiao and Huang, Kui and Mao, Shanjin and Li, Rugui and Dong, Haili and Zhai, Xi},
  title = {Recovery of Valuable Metals from Spent Lithium-Ion Batteries by Combining Reduction Roasting and Selective Leaching},
  journal = {Recycling},
  year = {2026},
  volume = {11},
  number = {3},
  pages = {59},
  doi = {10.3390/recycling11030059}
}
Kostenlos starten →