Kerosene Fraction from Polyethylene by Pressurized Thermal Pyrolysis and Hydroisomerization over a Pt/SAPO-11 Catalyst

Roman E. Yakovenko, Viktoria S. Marchenko, Danila A. Ponomarev, Denis A. Ponomarev, Anastasia A. Chemes, Maksim S. Zagordskikh, Marat R. Agliullin

Processes · 16.11.2026 · 14 (22) · 3688

DOI: 10.3390/pr14223688 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Processes, online erschienen am 16.11.2026. Verfasst von Roman E. Yakovenko und 6 weiteren Autor:innen. Die Arbeit nennt 40 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Ministry of Science and Higher Education of the Russian Federation.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Thermal pyrolysis of polyethylene (PE) under pressure and hydroisomerization over Pt/SAPO-11 are known separately; this work examines their integration. PE was pyrolyzed at 400–550 °C and constant pressures of 0.1–2.0 MPa, and the 140–280 °C fraction (pyrolysis kerosene) was hydroisomerized over 0.5 wt% Pt/SAPO-11. The yield of the 140–280 °C fraction decreases with temperature and increases with pressure, reaching 45.3 wt% at 400 °C and 1.0 MPa (27.4 wt% at 0.1 MPa); a control run under these conditions gave a directly measured gas yield of 13.2 wt% and a mass balance closure of 99.3%. The pyrolysis kerosene contains 47.6 wt% alkenes and 20.0 wt% cycloalkanes. Hydroisomerization at 6 MPa and a liquid hourly space velocity of 3 h−1 gives 91.1–93.4 wt% of the kerosene fraction (>140 °C) at 290–300 °C, with near-complete alkene hydrogenation; at 330 °C, the freezing point falls below −90 °C (pyrolysis kerosene: −13 °C), but hydrocracking reduces the yield to 72.4 wt%. The kerosene fraction obtained at the selected temperature of 300 °C (57.2% isoalkanes, 25.1% cycloalkanes, 0.1% aromatics) meets all measured GOST 10227-86 requirements for Russian RT jet fuel except density. The overall kerosene yield is 41.3 wt% of PE (40.0–40.4 wt% within the 140–280 °C boundaries). A preliminary estimate shows that the heat and hydrogen demand of the process corresponds to 68–97% of the energy of the pyrolysis gases.

Förderung

  • Ministry of Science and Higher Education of the Russian Federation

Zitieren

APA

Yakovenko, R. E., Marchenko, V. S., Ponomarev, D. A., Ponomarev, D. A., Chemes, A. A., Zagordskikh, M. S., & Agliullin, M. R. (2026). Kerosene Fraction from Polyethylene by Pressurized Thermal Pyrolysis and Hydroisomerization over a Pt/SAPO-11 Catalyst. Processes, 14(22), 3688. https://doi.org/10.3390/pr14223688

Vancouver

Yakovenko RE, Marchenko VS, Ponomarev DA, Ponomarev DA, Chemes AA, Zagordskikh MS, et al. Kerosene Fraction from Polyethylene by Pressurized Thermal Pyrolysis and Hydroisomerization over a Pt/SAPO-11 Catalyst. Processes. 2026;14(22):3688. doi:10.3390/pr14223688

BibTeX
@article{Yakovenko2026,
  author = {Yakovenko, Roman E. and Marchenko, Viktoria S. and Ponomarev, Danila A. and Ponomarev, Denis A. and Chemes, Anastasia A. and Zagordskikh, Maksim S. and Agliullin, Marat R.},
  title = {Kerosene Fraction from Polyethylene by Pressurized Thermal Pyrolysis and Hydroisomerization over a Pt/SAPO-11 Catalyst},
  journal = {Processes},
  year = {2026},
  volume = {14},
  number = {22},
  pages = {3688},
  doi = {10.3390/pr14223688}
}
Kostenlos starten →