Kurz gefasst

Fachartikel in der Zeitschrift Polysaccharides, online erschienen am 15.07.2026. Verfasst von José Javier Coca-Hidalgo und 4 weiteren Autor:innen. Die Arbeit wurde bisher 1-mal zitiert (Crossref) und nennt 54 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Secretaría de Ciencia, Humanidades, Tecnología e Innovación.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

This work is focused on understanding how the properties of chitosan-g-poly(N,N-diethylacrylamide-co-N,N-dimethylacrylamide) and chitosan-g-poly(N,N-diethylacrylamide-co-N-ethylacrylamide) copolymers are affected by varying their compositions. Poly(N,N-diethylacrylamide), PDEAm, is a thermosensitive polymer with a reversible coil-to-globule transition in aqueous solution near the human body temperature. The transition temperature can be tuned by varying the amount of two more hydrophilic units: N-ethylacrylamide (NEAm) or N,N-dimethylacrylamide (DMAm). While the former can participate in hydrogen bonding as a proton donor or acceptor, the latter is only an acceptor and a very-well-known hydrophilic unit with no phase transition. The gelation process was followed by rheological measurements, showing the general features of the chemical gelation and the formation of a strong gel. A reaction autoacceleration was observed, which is interpreted by the high viscosity of the reaction mixture due to the presence of chitosan, although a greater effect was found in NEAm copolymers due to the higher hydrogen-bonding capacity of NEAm. A relationship was found between the compositions of both copolymers, the strength of the hydrogels, and the calculated pore size. The pore sizes range from 32 to 18 nm. Thermogravimetric analysis of the hydrogels showed the typical decomposition stages of polyacrylamides. Neither the temperature of the maximum decomposition rate nor the weight loss associated displayed a clear trend with the copolymer composition. There was an increment in the equilibrium swelling values with the content of NEAm units (from 16 to almost 28 g water/g polymer), but the copolymers with DMAm remained unaffected (swelling values around 23 g water/g polymer). The hydrogen-bonding interaction affected the gelation process and swelling behavior of the hydrogels. This can be explained by the greater ability of NEAm to form hydrogen bonds compared to DMAm.

Förderung

  • Secretaría de Ciencia, Humanidades, Tecnología e Innovación

Zitieren

APA

Coca-Hidalgo, J. J., Silva-Gutiérrez, L., Peniche-Covas, C., Lizardi-Mendoza, J., & Argüelles-Monal, W. M. (2026). Synthesis and Characterization of Hydrogels Based on Chitosan-g-N-Alkyl-Substituted Polyacrylamide Copolymers. Polysaccharides, 7(3), 88. https://doi.org/10.3390/polysaccharides7030088

Vancouver

Coca-Hidalgo JJ, Silva-Gutiérrez L, Peniche-Covas C, Lizardi-Mendoza J, Argüelles-Monal WM. Synthesis and Characterization of Hydrogels Based on Chitosan-g-N-Alkyl-Substituted Polyacrylamide Copolymers. Polysaccharides. 2026;7(3):88. doi:10.3390/polysaccharides7030088

BibTeX
@article{CocaHidalgo2026,
  author = {Coca-Hidalgo, José Javier and Silva-Gutiérrez, Luisa and Peniche-Covas, Carlos and Lizardi-Mendoza, Jaime and Argüelles-Monal, Waldo Manuel},
  title = {Synthesis and Characterization of Hydrogels Based on Chitosan-g-N-Alkyl-Substituted Polyacrylamide Copolymers},
  journal = {Polysaccharides},
  year = {2026},
  volume = {7},
  number = {3},
  pages = {88},
  doi = {10.3390/polysaccharides7030088}
}
Kostenlos starten →