EUVIMEDEUVIMED entdecken
Open Access · CC BY 4.0

Thermal Aging of PFA-Insulated Aerospace Cables: Coupled Thermal Transport, Dielectric, and Breakdown Response

Jawad Ahmad, Mohamad Ghaffarian Niasar

Polymers · 20.11.2026 · 18 (22) · 2925

DOI: 10.3390/polym18222925 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Polymers, online erschienen am 20.11.2026. Verfasst von Jawad Ahmad und 1 weiteren Autor:innen. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Dutch Nationaal Groeifonds (NGF) through the Luchtvaart in Transitie program, under project STD1 Elektrische Kabelsystemen.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

The long-term reliability of fluoropolymer-insulated wiring is increasingly important for electrified aircraft operating under elevated thermal and electrical stress. This study investigates the aging behavior of full-scale perfluoroalkoxy (PFA)-insulated aircraft cable subjected to cyclic thermal exposure at 280 °C for a nominal duration of up to 1000 h, combining surface, thermal, dielectric, charge transport, AC breakdown, and finite-element analyses. The results reveal a two-stage aging response. During the early stage, up to approximately 500 h, thermal exposure promoted annealing and structural rearrangement, leading to improved thermal–dielectric stability and enhanced AC breakdown strength. At longer aging times, degradation-assisted rearrangement became more influential, producing increased structural heterogeneity, free volume, and easier charge transport. These changes were reflected in reduced thermal conductivity, altered transient heating and cooling behavior, increased permittivity, dielectric loss and conductivity, and reduced insulation resistance. High-temperature broadband dielectric spectroscopy showed a slight reduction in the activation energy for DC conduction after aging, while thermally stimulated depolarization current analysis indicated increased released charge and trap density, together with a reduction in trap depth from 1.42 to 0.95 eV after 1000 h, suggesting the formation of more numerous shallow trapping sites. Despite these changes, dielectric loss increased by only about 33% after 1000 h, indicating that severe dielectric deterioration had not occurred. AC breakdown strength followed the same two-stage behavior, increasing up to about 500 h before declining at longer aging times. Importantly, breakdown strength depended strongly on the electrically stressed insulation length; for the 1000 h cable, increasing the stressed length from 2.5 to 20 cm reduced breakdown strength from 26.6 to 21.4 kV/mm. Finite-element simulations further confirmed that aging-induced changes in thermal transport modify the transient heat dissipation response of the cable. Overall, PFA retained substantial thermal and dielectric functionality after 1000 h, while prolonged-aging-induced charge transport, shallow-trap formation, and stressed insulation length emerged as critical factors for assessing the long-term reliability of aircraft wiring systems.

Förderung

  • Dutch Nationaal Groeifonds (NGF) through the Luchtvaart in Transitie program, under project STD1 Elektrische Kabelsystemen

Zitieren

APA

Ahmad, J., & Niasar, M. G. (2026). Thermal Aging of PFA-Insulated Aerospace Cables: Coupled Thermal Transport, Dielectric, and Breakdown Response. Polymers, 18(22), 2925. https://doi.org/10.3390/polym18222925

Vancouver

Ahmad J, Niasar MG. Thermal Aging of PFA-Insulated Aerospace Cables: Coupled Thermal Transport, Dielectric, and Breakdown Response. Polymers. 2026;18(22):2925. doi:10.3390/polym18222925

BibTeX
@article{Ahmad2026,
  author = {Ahmad, Jawad and Niasar, Mohamad Ghaffarian},
  title = {Thermal Aging of PFA-Insulated Aerospace Cables: Coupled Thermal Transport, Dielectric, and Breakdown Response},
  journal = {Polymers},
  year = {2026},
  volume = {18},
  number = {22},
  pages = {2925},
  doi = {10.3390/polym18222925}
}