EUVIMEDEUVIMED entdecken
Open Access · CC BY 4.0

Thermal Pre-Aging-Dependent Seawater-Induced Degradation of XLPE Submarine Cable Insulation: Electrical Performance Evolution and Microstructural Mechanisms

Liang Zou iD, Shoushui Han, Zhiyun Han iD, Rongzhao Jia, Qingsong Liu, Zheng Liu iD, Hanwen Ren

Polymers · 16.07.2026 · 18 (14) · 1747

DOI: 10.3390/polym18141747 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Polymers, online erschienen am 16.07.2026. Verfasst von Liang Zou und 6 weiteren Autor:innen. Beteiligte Einrichtung: School of Electrical Engineering, Shandong University, Jinan 250061, China. Die Arbeit wurde bisher 1-mal zitiert (Crossref) und nennt 36 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: National Natural Science Foundation of China, China Southern Power Grid (China).

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

The long-term reliability of XLPE submarine cable insulation is influenced by progressive thermal degradation during operation and subsequent seawater ingress caused by external damage. Although thermal aging and seawater exposure have been widely investigated individually, the influence of the prior thermal-aging state on the subsequent seawater-induced degradation behavior of XLPE remains insufficiently understood. In this study, XLPE insulation specimens prepared from the same commercial compound used for 500 kV submarine cables were subjected to sequential accelerated aging consisting of controlled thermal pre-aging followed by simulated seawater exposure. Broadband dielectric spectroscopy, AC breakdown testing with two-parameter Weibull analysis, scanning electron microscopy (SEM), and Fourier-transform infrared spectroscopy (FTIR) were employed to investigate the evolution of electrical properties, surface morphology, and molecular structure. The results demonstrate that seawater-induced electrical deterioration strongly depends on the initial thermal-aging state of XLPE. Increasing thermal pre-aging duration resulted in progressively higher relative permittivity and dielectric loss, together with reduced characteristic breakdown strength after subsequent seawater exposure. Under the most severe condition of 1440 h thermal pre-aging followed by 672 h seawater exposure, the power–frequency relative permittivity increased by 32.1%, while the characteristic breakdown strength decreased by more than one-third compared with the initial state. SEM observations revealed that thermally pre-aged specimens developed accelerated surface damage during seawater exposure, including pores, cracks, corrosion pits, and honeycomb-like structures. FTIR analysis further indicated molecular-chain degradation and increased hydroxyl-related species during sequential aging. These results suggest that thermal-aging-induced molecular oxidation, polar-group formation, and microstructural defects enhance water and ion penetration pathways, thereby increasing the susceptibility of XLPE insulation to subsequent seawater-induced degradation. This study provides material-level experimental evidence for understanding sequential aging processes in submarine cable insulation and highlights the importance of considering historical thermal damage in future condition assessment and lifetime evaluation models. Since accelerated laboratory conditions were adopted, the results should be interpreted as comparative degradation characteristics rather than direct predictions of field-service lifetime.

Schlagwörter

Stichwörter der Autor:innen

cross-linked polyethyleneseawater corrosionsubmarine cablethermal agingtime-series coupling

Autor:innen und Institutionen

  • School of Electrical Engineering, Shandong University, Jinan 250061, China.
  • Research Institute of Electric Power, China Southern Power Grid Ultra-High Voltage Transmission Company, Guangzhou 510663, China.
  • State Key Laboratory of Alternate Electrical Power System with Renewable Energy Sources, North China Electric Power University, Beijing 100096, China.

ORCID-Profile: Liang Zou, Zhiyun Han, Zheng Liu

Förderung

  • National Natural Science Foundation of China
  • China Southern Power Grid (China)

Zitieren

APA

Zou, L., Han, S., Han, Z., Jia, R., Liu, Q., Liu, Z., & Ren, H. (2026). Thermal Pre-Aging-Dependent Seawater-Induced Degradation of XLPE Submarine Cable Insulation: Electrical Performance Evolution and Microstructural Mechanisms. Polymers, 18(14), 1747. https://doi.org/10.3390/polym18141747

Vancouver

Zou L, Han S, Han Z, Jia R, Liu Q, Liu Z, et al. Thermal Pre-Aging-Dependent Seawater-Induced Degradation of XLPE Submarine Cable Insulation: Electrical Performance Evolution and Microstructural Mechanisms. Polymers. 2026;18(14):1747. doi:10.3390/polym18141747

BibTeX
@article{Zou2026,
  author = {Zou, Liang and Han, Shoushui and Han, Zhiyun and Jia, Rongzhao and Liu, Qingsong and Liu, Zheng and Ren, Hanwen},
  title = {Thermal Pre-Aging-Dependent Seawater-Induced Degradation of XLPE Submarine Cable Insulation: Electrical Performance Evolution and Microstructural Mechanisms},
  journal = {Polymers},
  year = {2026},
  volume = {18},
  number = {14},
  pages = {1747},
  doi = {10.3390/polym18141747}
}