Fachartikel in der Zeitschrift Polymers, online erschienen am 24.06.2026. Verfasst von Nitesh Subedi und 5 weiteren Autor:innen. Beteiligte Einrichtung: School of Aerospace and Mechanical Engineering, University of Oklahoma, Norman, OK 73019, USA. Die Arbeit wurde bisher 1-mal zitiert (Crossref) und nennt 24 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0).
Abstract (Originalsprache)
Hydrogen-compatible elastomeric seals are critical for the reliability and safety of high-pressure hydrogen infrastructure. However, hydrogen exposure can alter the mechanical response and surface condition of elastomeric materials through coupled transport–mechanical interactions. This study presents a comparative experimental and data-driven investigation of the pressure-dependent degradation behavior of ethylene propylene diene monomer (EPDM), nitrile butadiene rubber (NBR), and fluorocarbon elastomer (FKM) O-ring seals following 192 h exposure to hydrogen pressures ranging from 800 to 7000 psi at room temperature. Tensile testing was performed directly on complete O-ring geometries, and descriptor-based analysis was used to quantify peak-response behavior, energy absorption, stiffness evolution, and normalized deformation characteristics. Multivariate statistical methods, principal component analysis (PCA), clustering analysis, and Random Forest regression were applied to identify material-specific degradation patterns. NBR maintained the highest overall load-bearing capability and stiffness-related response across the investigated pressure range, whereas EPDM exhibited more compliant and non-monotonic deformation behavior. FKM showed the strongest pressure sensitivity, with substantial increases in force- and stiffness-related descriptors at elevated hydrogen pressures. Optical image analysis revealed pronounced increases in defect density and defect area fraction for NBR, while FKM exhibited comparatively stable surface-state behavior. PCA and clustering analyses identified distinct material-dependent degradation trajectories, and Random Forest regression achieved an R2 value of 0.888 for energy-absorption prediction. The results demonstrate that hydrogen-induced degradation emerges through coupled interactions among stiffness evolution, deformation progression, energy absorption, and surface-state changes, providing a comparative framework for assessing elastomer performance in hydrogen environments.
Schlagwörter
Stichwörter der Autor:innen
Autor:innen und Institutionen
- School of Aerospace and Mechanical Engineering, University of Oklahoma, Norman, OK 73019, USA.
ORCID-Profile: Nitesh Subedi, Md Monjur Hossain Bhuiyan, Omkar Gautam, Zahed Siddique
Zitieren
APA
Subedi, N., Becerril Corral, A., Bhuiyan, M. M. H., Gautam, O., Islam, M. A., & Siddique, Z. (2026). Data-Driven Multivariate Characterization of Hydrogen-Induced Response Evolution in EPDM, NBR, and FKM Elastomers. Polymers, 18(13), 1570. https://doi.org/10.3390/polym18131570
Vancouver
Subedi N, Becerril Corral A, Bhuiyan MMH, Gautam O, Islam MA, Siddique Z. Data-Driven Multivariate Characterization of Hydrogen-Induced Response Evolution in EPDM, NBR, and FKM Elastomers. Polymers. 2026;18(13):1570. doi:10.3390/polym18131570
BibTeX
@article{Subedi2026,
author = {Subedi, Nitesh and Becerril Corral, Alfredo and Bhuiyan, Md Monjur Hossain and Gautam, Omkar and Islam, Md Ariful and Siddique, Zahed},
title = {Data-Driven Multivariate Characterization of Hydrogen-Induced Response Evolution in EPDM, NBR, and FKM Elastomers},
journal = {Polymers},
year = {2026},
volume = {18},
number = {13},
pages = {1570},
doi = {10.3390/polym18131570}
}
EUVIMED