Hollow Auxetic Polymer Structures with Manufacturing-Constrained Design and Mechanical Validation
Polymers · 28.03.2026 · 18 (7) · 828
DOI: 10.3390/polym18070828 ↗Kurz gefasst
Fachartikel in der Zeitschrift Polymers, online erschienen am 28.03.2026. Verfasst von Finlay Bridge und 3 weiteren Autor:innen. Beteiligte Einrichtung: Mechanical Engineering, University of Birmingham, Edgbaston, Birmingham B15 2TT, UK. Die Arbeit wurde bisher 1-mal zitiert (Crossref) und nennt 45 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Umm Al-Qura University, Umm Al-Qura University https://ror.org/01xjqrm90.
Abstract (Originalsprache)
Hollow auxetic structures enable lightweight mechanical design by reducing mass while preserving architected deformation. However, hollow auxetic studies focus on LPBF metals. This study presents a manufacturing-constrained design and validation framework for a hollow hybrid re-entrant chiral lattice produced by stereolithography. The unit cell was parameterised by chiral angle, re-entrant strut length, and hollow internal diameter, with drainage features integrated into the CAD model to preserve hollow channels during printing and post-processing. A minimum internal diameter study defined the printable design window. Within these limits, a central composite design coupled with finite element analysis mapped the response surface and identified an optimised geometry of θ = 15°, L = 3.5 mm, and d = 1.68 mm, with a predicted unit-cell negative Poisson’s ratio of about −1.17. Compression testing confirmed that the printed unit cell and 3 × 3 × 3 lattice retained the intended rotation-dominated auxetic deformation mode. At the selected comparison strain, the unit cell showed a negative Poisson’s ratio of −0.68 and the 3 × 3 × 3 lattice showed −0.29. Relative to the solid lattice, the hollow lattice reduced density by 42.4% with only a 3.0% reduction in stiffness, increasing specific stiffness by 68.9% and specific peak strength by 5.2%, but reducing specific energy absorption by 25.6% due to earlier localisation and junction driven fracture. These results provide practical design guidance for manufacturable hollow SLA auxetic lattices, especially for lightweight and stiffness-limited applications where low mass and high specific stiffness are more important than energy absorption.
Schlagwörter
Stichwörter der Autor:innen
Autor:innen und Institutionen
- Mechanical Engineering, University of Birmingham, Edgbaston, Birmingham B15 2TT, UK.
- Industrial Engineering Department, College of Engineering and Architecture, Umm Al-Qura University, Makkah 21955, Saudi Arabia.
- School of Sciences, Psychology, Arts and Humanities, Computing, Engineering, and Sport, Canterbury Christ Church University, Canterbury CT1 1QU, UK.
ORCID-Profile: Rakan Albarakati, Hany Hassanin, Khamis Essa
Förderung
- Umm Al-Qura University
- Umm Al-Qura University https://ror.org/01xjqrm90
Zitieren
APA
Bridge, F., Albarakati, R., Hassanin, H., & Essa, K. (2026). Hollow Auxetic Polymer Structures with Manufacturing-Constrained Design and Mechanical Validation. Polymers, 18(7), 828. https://doi.org/10.3390/polym18070828
Vancouver
Bridge F, Albarakati R, Hassanin H, Essa K. Hollow Auxetic Polymer Structures with Manufacturing-Constrained Design and Mechanical Validation. Polymers. 2026;18(7):828. doi:10.3390/polym18070828
BibTeX
@article{Bridge2026,
author = {Bridge, Finlay and Albarakati, Rakan and Hassanin, Hany and Essa, Khamis},
title = {Hollow Auxetic Polymer Structures with Manufacturing-Constrained Design and Mechanical Validation},
journal = {Polymers},
year = {2026},
volume = {18},
number = {7},
pages = {828},
doi = {10.3390/polym18070828}
}
EUVIMED