The Influence of Oil and Thermal Aging on the Sealing Characteristics of NBR Seals
Polymers · 02.09.2024 · 16 (17) · 2501
DOI: 10.3390/polym16172501 ↗Kurz gefasst
Fachartikel in der Zeitschrift Polymers, online erschienen am 02.09.2024. Verfasst von Yiding Li und 5 weiteren Autor:innen. Beteiligte Einrichtung: Center for Rubber Composite Materials and Structures, Harbin Institute of Technology, Weihai 264209, China. Die Arbeit wurde bisher 25-mal zitiert (Crossref) und nennt 53 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Science Foundation of National Key Laboratory of Science and Technology on Advanced Compo-sites in Special Environments, National Key Laboratory of Science and Technology on Advanced Composites in Special Environments.
Abstract (Originalsprache)
Nitrile Butadiene Rubber (NBR) is widely used as a sealing material due to its excellent mechanical properties and good oil resistance. However, when using NBR material, the seal structure is unable to avoid the negative effects of rubber aging. Hence, the influence of oil and thermal aging on the characteristics of NBR seals was studied by coupling the mechanical behavioral changes with the tribological behavioral changes of NBR in oil and the thermal environment. For this paper, aging testing and compression testing of NBR were carried out. Additionally, friction testing between friction pairs under different aging times was carried out. The surface morphology of the NBR working surface under different aging conditions was also observed. Finally, coefficients of different test conditions were introduced into the finite element model of NBR seals. It can be seen from the results that the elastic modulus increased with the increase in aging time in the thermal oxidative aging testing. The elastic modulus after 7 days of thermal oxidative aging increased by 135.45% compared to the unaged case, and the elastic modulus after 7 days of oil aging increased by 15.03% compared to the unaged case. The compression set rate of NBR increased significantly with the increase in aging time and temperature. The coefficient of friction (COF) between friction pairs increased first and then decreased with the increase in aging time. The maximum contact pressure decreased by 2.43% between the shaft and sealing ring and decreased by 4.01% between the O-ring and groove. The proportion of the effective sealing area decreased by 3.05% between the shaft and sealing ring and decreased by 6.11% between the O-ring and groove. Furthermore, the sealing characteristics between the O-ring and groove were better than those between the shaft and sealing ring.
Schlagwörter
Stichwörter der Autor:innen
Autor:innen und Institutionen
- Center for Rubber Composite Materials and Structures, Harbin Institute of Technology, Weihai 264209, China.
- National Key Laboratory of Science and Technology on Advanced Composites in Special Environments, Harbin Institute of Technology, Harbin 150090, China.
ORCID-Profile: Jian Wu, Benlong Su
Förderung
- Science Foundation of National Key Laboratory of Science and Technology on Advanced Compo-sites in Special Environments
- National Key Laboratory of Science and Technology on Advanced Composites in Special Environments
Zitieren
APA
Li, Y., Wu, J., Chen, Z., Zhang, Z., Su, B., & Wang, Y. (2024). The Influence of Oil and Thermal Aging on the Sealing Characteristics of NBR Seals. Polymers, 16(17), 2501. https://doi.org/10.3390/polym16172501
Vancouver
Li Y, Wu J, Chen Z, Zhang Z, Su B, Wang Y. The Influence of Oil and Thermal Aging on the Sealing Characteristics of NBR Seals. Polymers. 2024;16(17):2501. doi:10.3390/polym16172501
BibTeX
@article{Li2024,
author = {Li, Yiding and Wu, Jian and Chen, Zhihao and Zhang, Ziqi and Su, Benlong and Wang, Youshan},
title = {The Influence of Oil and Thermal Aging on the Sealing Characteristics of NBR Seals},
journal = {Polymers},
year = {2024},
volume = {16},
number = {17},
pages = {2501},
doi = {10.3390/polym16172501}
}
EUVIMED