Fachartikel in der Zeitschrift Polymers, online erschienen am 16.06.2024. Verfasst von Jaemin Son und 5 weiteren Autor:innen. Beteiligte Einrichtung: Department of Textile System Engineering, Kyungpook National University, Daegu 41566, Republic of Korea. Die Arbeit wurde bisher 10-mal zitiert (Crossref) und nennt 39 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Kyungpook National University, Kyungpook National University Research Fund.
Abstract (Originalsprache)
Polymers with a low dielectric constant (Dk) are promising materials for high-speed communication networks, which demand exceptional thermal stability, ultralow Dk and dissipation factor, and minimum moisture absorption. In this paper, we prepared a series of novel low-Dk polyimide films containing an MCM-41-type amino-functionalized mesoporous silica (AMS) via in situ polymerization and subsequent thermal imidization and investigated their morphologies, thermal properties, frequency-dependent dielectric behaviors, and water permeabilities. Incorporating 6 wt.% AMS reduced the Dk at 1 MHz from 2.91 of the pristine fluorinated polyimide (FPI) to 2.67 of the AMS-grafted FPI (FPI-g-AMS), attributed to the free volume and low polarizability of fluorine moieties in the backbone and the incorporation of air voids within the mesoporous AMS particles. The FPI-g-AMS films presented a stable dissipation factor across a wide frequency range. Introducing a silane coupling agent increased the hydrophobicity of AMS surfaces, which inhibited the approaching of the water molecules, avoiding the hydrolysis of Si–O–Si bonds of the AMS pore walls. The increased tortuosity caused by the AMS particles also reduced water permeability. All the FPI-g-AMS films displayed excellent thermooxidative/thermomechanical stability, including a high 5% weight loss temperature (>531 °C), char residue at 800 °C (>51%), and glass transition temperature (>300 °C).
Schlagwörter
Stichwörter der Autor:innen
Autor:innen und Institutionen
- Department of Textile System Engineering, Kyungpook National University, Daegu 41566, Republic of Korea.
Förderung
- Kyungpook National University
- Kyungpook National University Research Fund
Zitieren
APA
Son, J., Park, H., Kim, M., Park, J. H., Nam, K. H., & Bae, J. S. (2024). Frequency-Dependent Dielectric Permittivity and Water Permeability in Ordered Mesoporous Silica-Grafted Fluorinated Polyimides. Polymers, 16(12), 1716. https://doi.org/10.3390/polym16121716
Vancouver
Son J, Park H, Kim M, Park JH, Nam KH, Bae JS. Frequency-Dependent Dielectric Permittivity and Water Permeability in Ordered Mesoporous Silica-Grafted Fluorinated Polyimides. Polymers. 2024;16(12):1716. doi:10.3390/polym16121716
BibTeX
@article{Son2024,
author = {Son, Jaemin and Park, Hwon and Kim, Minju and Park, Jae Hui and Nam, Ki-Ho and Bae, Jin-Seok},
title = {Frequency-Dependent Dielectric Permittivity and Water Permeability in Ordered Mesoporous Silica-Grafted Fluorinated Polyimides},
journal = {Polymers},
year = {2024},
volume = {16},
number = {12},
pages = {1716},
doi = {10.3390/polym16121716}
}
EUVIMED