Accelerated Degradation of Poly-ε-caprolactone Composite Scaffolds for Large Bone Defects
Polymers · 28.01.2023 · 15 (3) · 670
DOI: 10.3390/polym15030670 ↗Kurz gefasst
Fachartikel in der Zeitschrift Polymers, online erschienen am 28.01.2023. Verfasst von Evangelos Daskalakis und 9 weiteren Autor:innen. Beteiligte Einrichtung: School of Mechanical, Aerospace and Civil Engineering, University of Manchester, Manchester M13 9PL, UK. Die Arbeit wurde bisher 49-mal zitiert (Crossref) und nennt 67 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Engineering and Physical Sciences Research Council, University of Manchester.
Abstract (Originalsprache)
This research investigates the accelerated hydrolytic degradation process of both anatomically designed bone scaffolds with a pore size gradient and a rectangular shape (biomimetically designed scaffolds or bone bricks). The effect of material composition is investigated considering poly-ε-caprolactone (PCL) as the main scaffold material, reinforced with ceramics such as hydroxyapatite (HA), β-tricalcium phosphate (TCP) and bioglass at a concentration of 20 wt%. In the case of rectangular scaffolds, the effect of pore size (200 μm, 300 μm and 500 μm) is also investigated. The degradation process (accelerated degradation) was investigated during a period of 5 days in a sodium hydroxide (NaOH) medium. Degraded bone bricks and rectangular scaffolds were measured each day to evaluate the weight loss of the samples, which were also morphologically, thermally, chemically and mechanically assessed. The results show that the PCL/bioglass bone brick scaffolds exhibited faster degradation kinetics in comparison with the PCL, PCL/HA and PCL/TCP bone bricks. Furthermore, the degradation kinetics of rectangular scaffolds increased by increasing the pore size from 500 μm to 200 μm. The results also indicate that, for the same material composition, bone bricks degrade slower compared with rectangular scaffolds. The scanning electron microscopy (SEM) images show that the degradation process was faster on the external regions of the bone brick scaffolds (600 μm pore size) compared with the internal regions (200 μm pore size). The thermal gravimetric analysis (TGA) results show that the ceramic concentration remained constant throughout the degradation process, while differential scanning calorimetry (DSC) results show that all scaffolds exhibited a reduction in crystallinity (Xc), enthalpy (Δm) and melting temperature (Tm) throughout the degradation process, while the glass transition temperature (Tg) slightly increased. Finally, the compression results show that the mechanical properties decreased during the degradation process, with PCL/bioglass bone bricks and rectangular scaffolds presenting higher mechanical properties with the same design in comparison with the other materials.
Schlagwörter
Stichwörter der Autor:innen
Autor:innen und Institutionen
- School of Mechanical, Aerospace and Civil Engineering, University of Manchester, Manchester M13 9PL, UK.
- Integrated Manufacturing Technologies Research and Application Center, Sabanci University, Tuzla 34956, Istanbul, Turkey.
- SUNUM Nanotechnology Research Center, Sabanci University, Tuzla 34956, Istanbul, Turkey.
- Faculty of Engineering and Natural Sciences, Sabanci University, Tuzla 34956, Istanbul, Turkey.
- School of Pharmacy and Biomedical Sciences, University of Portsmouth, Portsmouth PO1 2DT, UK.
- Singapore Centre for 3D Printing, School of Mechanical and Aerospace Engineering, Nanyang Technological University, Singapore 639798, Singapore.
ORCID-Profile: Evangelos Daskalakis, Mohamed H Hassan, Ali Fallah, Glen Cooper, Andrew Weightman, Gordon Blunn, Bahattin Koc
Förderung
- Engineering and Physical Sciences Research Council
- University of Manchester
Zitieren
APA
Daskalakis, E., Hassan, M. H., Omar, A. M., Acar, A. A., Fallah, A., Cooper, G., Weightman, A., Blunn, G., Koc, B., & Bartolo, P. (2023). Accelerated Degradation of Poly-ε-caprolactone Composite Scaffolds for Large Bone Defects. Polymers, 15(3), 670. https://doi.org/10.3390/polym15030670
Vancouver
Daskalakis E, Hassan MH, Omar AM, Acar AA, Fallah A, Cooper G, et al. Accelerated Degradation of Poly-ε-caprolactone Composite Scaffolds for Large Bone Defects. Polymers. 2023;15(3):670. doi:10.3390/polym15030670
BibTeX
@article{Daskalakis2023,
author = {Daskalakis, Evangelos and Hassan, Mohamed H and Omar, Abdalla M and Acar, Anil A and Fallah, Ali and Cooper, Glen and Weightman, Andrew and Blunn, Gordon and Koc, Bahattin and Bartolo, Paulo},
title = {Accelerated Degradation of Poly-ε-caprolactone Composite Scaffolds for Large Bone Defects},
journal = {Polymers},
year = {2023},
volume = {15},
number = {3},
pages = {670},
doi = {10.3390/polym15030670}
}