Highly Reversible Zn Anodes through a Hydrophobic Interface Formed by Electrolyte Additive

Xiaoying Yan, Yunwei Tong, Yingjie Liu, Xinyu Li, Zhenbo Qin, Zhong Wu iD, Wenbin Hu

Nanomaterials · 05.05.2023 · 13 (9) · 1547

DOI: 10.3390/nano13091547 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Nanomaterials, online erschienen am 05.05.2023. Verfasst von Xiaoying Yan und 6 weiteren Autor:innen. Beteiligte Einrichtung: School of Materials Science and Engineering, Tianjin Key Laboratory of Composite and Functional Materials, Key Laboratory of Advanced Ceramics and Ma…. Die Arbeit wurde bisher 9-mal zitiert (Crossref) und nennt 35 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: National Natural Science Foundation of China, Natural Science Foundation of Tianjin.

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Hydrogen evolution reaction and dendrite growth seriously break the Zn plating/stripping process at the electrolyte/electrode interface, causing the instability of the Zn anode of aqueous zinc ion batteries. To improve the Zn anode stability and reversibility, we report a new electrolyte additive of aqueous electrolyte with the hydrophobic group. This interfacial hydrophobicity maximises the exclusion of free water from the Zn anode surface, which blocks water erosion and reduces interfacial side reactions. Thus, in an optimal 2 M ZnSO4 electrolyte with 2 g·L−1 Tween-85, the hydrogen evolution reaction and other water-induced undesired reactions can be suppressed, which greatly improves the cycling stability and Coulombic efficiency (CE) of Zn plating/stripping process. The stable cycle time of the Zn//Zn symmetric battery reaches over 1300 h, especially at a high current density and a high areal capacity (more than 650 h at 5 mA·cm−2, 5 mAh·cm−2). The average Coulomb efficiency (CE) of Zn//Ti asymmetric cell achieves 98.11% after 300 cycles. The capacity retention rate of Zn//MnO2 full battery is up to 88.6% after 1000 cycles.

Schlagwörter

Stichwörter der Autor:innen

HERZinc-ion batteriesaqueous electrolyteselectrolyte additivehydrophobicity

Autor:innen und Institutionen

  • School of Materials Science and Engineering, Tianjin Key Laboratory of Composite and Functional Materials, Key Laboratory of Advanced Ceramics and Machining Technology (Ministry of Education), Tianjin University, Tianji…
  • Joint School of National University of Singapore and Tianjin University, International Campus of Tianjin University, Fuzhou 350207, China.

ORCID-Profile: Zhong Wu

Förderung

  • National Natural Science Foundation of China
  • Natural Science Foundation of Tianjin

Zitieren

APA

Yan, X., Tong, Y., Liu, Y., Li, X., Qin, Z., Wu, Z., & Hu, W. (2023). Highly Reversible Zn Anodes through a Hydrophobic Interface Formed by Electrolyte Additive. Nanomaterials, 13(9), 1547. https://doi.org/10.3390/nano13091547

Vancouver

Yan X, Tong Y, Liu Y, Li X, Qin Z, Wu Z, et al. Highly Reversible Zn Anodes through a Hydrophobic Interface Formed by Electrolyte Additive. Nanomaterials. 2023;13(9):1547. doi:10.3390/nano13091547

BibTeX
@article{Yan2023,
  author = {Yan, Xiaoying and Tong, Yunwei and Liu, Yingjie and Li, Xinyu and Qin, Zhenbo and Wu, Zhong and Hu, Wenbin},
  title = {Highly Reversible Zn Anodes through a Hydrophobic Interface Formed by Electrolyte Additive},
  journal = {Nanomaterials},
  year = {2023},
  volume = {13},
  number = {9},
  pages = {1547},
  doi = {10.3390/nano13091547}
}
Kostenlos starten →