Effects of Alkali Metal Impurities on the High-Temperature Performance of Quartz Components: From Local Network Modification to Component Degradation
Minerals · 20.11.2026 · 16 (11) · 1210
DOI: 10.3390/min16111210 ↗Kurz gefasst
Fachartikel in der Zeitschrift Minerals, online erschienen am 20.11.2026. Verfasst von Hongjie Wang und 2 weiteren Autor:innen. Die Arbeit nennt 38 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: National Key R&D Program for Strategic Mineral Resources Development and Utilization, Chinese Academy of Sciences.
Abstract (Originalsprache)
Quartz and silica glass derive their high viscosity, low thermal expansion, and excellent thermal shock resistance from a continuous framework of SiO4 tetrahedra. Although Li, Na and K impurities are generally present at low concentrations, their effects are not simply proportional to the total abundance. Instead, their influence depends on structural location, coupling with Al and OH, surface enrichment, and high-temperature exposure time. Alkalis do more than lower a nominal melting temperature: they modify, or accompany changes in, the defect chemistry of the Si–O network. In crystalline quartz feedstocks, they may compensate the effective negative charge of substitutional Al defects or occur in inclusions and microcracks; after fusion, some may act as network modifiers that stabilize non-bridging oxygen. These processes can reduce high-temperature viscosity and creep resistance, accelerate ion migration and interfacial reactions, and interact with OH, bubbles, and cristobalite formation, ultimately contributing to deformation, dimensional drift, embrittlement, spalling, or process contamination. This review distinguishes crystalline quartz from fused quartz and silica glass and examines the links among non-bridging oxygen formation, local network depolymerization, viscosity, ionic transport, crystallization, and bubble evolution. Differences among alkalis, component-level degradation, analytical strategies, and engineering controls are also discussed. Silica glass has no single fixed melting point that adequately describes its service-temperature capability. Engineering assessment therefore requires viscosity–temperature relationships, strain and annealing points, softening behavior, creep, OH content, devitrification, bubble evolution, and surface contamination to be considered together.
Förderung
- National Key R&D Program for Strategic Mineral Resources Development and Utilization
- Chinese Academy of Sciences
Zitieren
APA
Wang, H., Zhou, Y., & Yang, X. (2026). Effects of Alkali Metal Impurities on the High-Temperature Performance of Quartz Components: From Local Network Modification to Component Degradation. Minerals, 16(11), 1210. https://doi.org/10.3390/min16111210
Vancouver
Wang H, Zhou Y, Yang X. Effects of Alkali Metal Impurities on the High-Temperature Performance of Quartz Components: From Local Network Modification to Component Degradation. Minerals. 2026;16(11):1210. doi:10.3390/min16111210
BibTeX
@article{Wang2026,
author = {Wang, Hongjie and Zhou, Yingjia and Yang, Xiaoyong},
title = {Effects of Alkali Metal Impurities on the High-Temperature Performance of Quartz Components: From Local Network Modification to Component Degradation},
journal = {Minerals},
year = {2026},
volume = {16},
number = {11},
pages = {1210},
doi = {10.3390/min16111210}
}