EUVIMEDEUVIMED entdecken
Open Access · CC BY 4.0

Investigation of Low-Temperature Cu/Cu Wafer Bonding with Sequential Plasma Activation for Hybrid Bonding

Junsha Wang, Kai Takeuchi, Michitaka Kubota, Masaya Kawano, Takeshi Takagi, Masaaki Niwa, Tadahiro Kuroda, Tadatomo Suga

Micromachines · 20.11.2026 · 17 (11) · 1348

DOI: 10.3390/mi17111348 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Micromachines, online erschienen am 20.11.2026. Verfasst von Junsha Wang und 7 weiteren Autor:innen. Die Arbeit nennt 39 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: New Energy and Industrial Technology Development Organization, Precise Measurement Technology Promotion Foundation.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

4-inch Cu/Cu wafer bonding with sequential plasma activation was investigated at 200 °C, and the effects of bonding atmosphere and Cu grain size on the bonding were investigated. With sequential plasma activation, the bonding atmosphere primarily affected the thickness of the interfacial oxide layer and may also have influenced its composition at the normal-grain Cu/Cu bonded interface. When bonding was performed in air, the interfacial oxide layer was approximately 80 nm thick and consisted mainly of Cu2O, with XPS suggesting a small amount of CuO on the debonded surfaces. In contrast, for bonding conducted under a vacuum of 1000 Pa, an approximately 10 nm thick Cu2O layer was observed. Although their bond strengths were comparable, wafer fracture during bond strength measurements of the vacuum-bonded Cu/Cu wafers suggested stronger interfacial bonding. With Ar ion beam treatment combined with sequential plasma activation, Cu grain size greatly affected the bonded interface. For fine-grain Cu wafers with grain size smaller than 100 nm, an oxide-free and nitride-free bonded interface was obtained, and Cu grain growth across the interface occurred, leading to strong interfacial bonding. However, for normal-grain Cu wafers with grain size of 200 nm–600 nm, an approximately 15 nm thick Cu2O layer was found at the bonded interface, and the bond strength was as low as 0.6 J/m2.

Förderung

  • New Energy and Industrial Technology Development Organization
  • Precise Measurement Technology Promotion Foundation

Zitieren

APA

Wang, J., Takeuchi, K., Kubota, M., Kawano, M., Takagi, T., Niwa, M., Kuroda, T., & Suga, T. (2026). Investigation of Low-Temperature Cu/Cu Wafer Bonding with Sequential Plasma Activation for Hybrid Bonding. Micromachines, 17(11), 1348. https://doi.org/10.3390/mi17111348

Vancouver

Wang J, Takeuchi K, Kubota M, Kawano M, Takagi T, Niwa M, et al. Investigation of Low-Temperature Cu/Cu Wafer Bonding with Sequential Plasma Activation for Hybrid Bonding. Micromachines. 2026;17(11):1348. doi:10.3390/mi17111348

BibTeX
@article{Wang2026,
  author = {Wang, Junsha and Takeuchi, Kai and Kubota, Michitaka and Kawano, Masaya and Takagi, Takeshi and Niwa, Masaaki and Kuroda, Tadahiro and Suga, Tadatomo},
  title = {Investigation of Low-Temperature Cu/Cu Wafer Bonding with Sequential Plasma Activation for Hybrid Bonding},
  journal = {Micromachines},
  year = {2026},
  volume = {17},
  number = {11},
  pages = {1348},
  doi = {10.3390/mi17111348}
}