Fachartikel in der Zeitschrift Micromachines, online erschienen am 17.05.2026. Verfasst von Gyuseong Chu und 1 weiteren Autor:innen. Beteiligte Einrichtung: Department of Materials Science and Engineering, College of Engineering, Korea National University of Transportation, Chungju 27469, Republic of Kore…. Die Arbeit nennt 22 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Korea RIC Association, Ministry of Education.

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Single-phase Cu4Bi4Se9 was successfully synthesized through a simple and rapid process combining mechanical alloying (MA) and hot pressing (HP). The phase formation behavior, microstructural evolution, charge transport characteristics, and thermoelectric properties were systematically investigated. X-ray diffraction analysis as a function of MA time confirmed that all powders crystallized into a single orthorhombic phase with space group Pnma. No decompositions or secondary phases were observed after HP sintering, indicating high phase stability. Thermogravimetric and differential scanning calorimetric analyses revealed distinct endothermic peaks at 714–717 K for all samples, corresponding to the onset of the decomposition of Cu4Bi4Se9. Microstructural observations showed that the relative density decreased with increasing HP temperature (>573 K), accompanied by grain growth and pore formation, reflecting the competition between Cu–Se interdiffusion and pore coarsening during high-temperature sintering. Hall effect measurements indicated p-type conduction for all samples, with carrier concentrations on the order of 1017 cm−3 and carrier mobilities of approximately 102 cm2 V−1 s−1. With increasing temperature, the electrical conductivity increased monotonically, while the Seebeck coefficient gradually decreased, resulting in a maximum power factor of 0.12 mW m−1 K−2 at 573 K. The total thermal conductivity remained extremely low, ranging from 0.33 to 0.48 W m−1 K−1, with the electronic contribution accounting for less than 10%, indicating that lattice thermal transport is dominant. The suppressed lattice thermal conductivity is attributed to the combined effects of Cu atomic rattling, asymmetric bonding induced by Bi 6s2 lone-pair electrons, and strong anharmonic phonon scattering arising from the complex crystal structure. Consequently, Cu4Bi4Se9 achieved a peak dimensionless figure of merit ZT of 0.19 in the temperature range of 573–623 K, demonstrating that the MA–HP process enables stable phase formation and competitive thermoelectric performance without post-annealing.

Schlagwörter

Stichwörter der Autor:innen

Cu4Bi4Se9hot pressingmechanical alloyingthermoelectric

Autor:innen und Institutionen

  • Department of Materials Science and Engineering, College of Engineering, Korea National University of Transportation, Chungju 27469, Republic of Korea.

ORCID-Profile: Il-Ho Kim

Förderung

  • Korea RIC Association
  • Ministry of Education

Zitieren

APA

Chu, G., & Kim, I. H. (2026). Thermoelectric Transport Properties of Cu4Bi4Se9 Prepared by Mechanical Alloying and Hot Pressing. Micromachines, 17(5), 615. https://doi.org/10.3390/mi17050615

Vancouver

Chu G, Kim IH. Thermoelectric Transport Properties of Cu4Bi4Se9 Prepared by Mechanical Alloying and Hot Pressing. Micromachines. 2026;17(5):615. doi:10.3390/mi17050615

BibTeX
@article{Chu2026,
  author = {Chu, Gyuseong and Kim, Il-Ho},
  title = {Thermoelectric Transport Properties of Cu4Bi4Se9 Prepared by Mechanical Alloying and Hot Pressing},
  journal = {Micromachines},
  year = {2026},
  volume = {17},
  number = {5},
  pages = {615},
  doi = {10.3390/mi17050615}
}
Kostenlos starten →