The Interplay of Core Diameter and Diameter Ratio on the Magnetic Properties of Bistable Glass-Coated Microwires
Micromachines · 22.10.2024 · 15 (11) · 1284
DOI: 10.3390/mi15111284 ↗Kurz gefasst
Fachartikel in der Zeitschrift Micromachines, online erschienen am 22.10.2024. Verfasst von Valeria Kolesnikova und 4 weiteren Autor:innen. Beteiligte Einrichtung: Research and Education Center "Smart Materials and Biomedical Applications", Immanuel Kant Baltic Federal University, 236041 Kaliningrad, Russia. Die Arbeit wurde bisher 3-mal zitiert (Crossref) und nennt 27 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Immanuel Kant Baltic Federal University.
Abstract (Originalsprache)
Glass-coated microwires exhibiting magnetic bistability have garnered significant attention as promising wireless sensing elements, primarily due to their rapid magnetization switching capabilities. These microwires consist of a metallic core with diameter d, encased in a glass coating, with a total diameter D. In this study, we investigated how the dimensions of both components and their ratio (d/D) influence the magnetization reversal behavior of Fe-based microwires. While previous studies have focused on either d or d/D individually, our research uniquely considered the combined effect of both parameters to provide a comprehensive understanding of their impact on magnetic properties. The metallic core diameter d varied from 10 to 19 µm and the d/D ratio was in the range of 0.48–0.68. To assess the magnetic properties of these microwires, including the shape of the hysteresis loop, coercivity, remanent magnetization, and the critical length of bistability, we employed vibrating sample magnetometry in conjunction with FORC-analysis. Additionally, to determine the critical length of bistability, magnetic measurements were conducted on microwires with various lengths, ranging from 1.5 cm down to 0.05 cm. Our findings reveal that coercivity is primarily dependent on the d/D parameter. These observations are effectively explained through an analysis that considers the competition between magnetostatic and magnetoelastic anisotropy energies. This comprehensive study paves the way for the tailored design of glass-coated microwires for diverse wireless sensing applications.
Schlagwörter
Stichwörter der Autor:innen
Autor:innen und Institutionen
- Research and Education Center "Smart Materials and Biomedical Applications", Immanuel Kant Baltic Federal University, 236041 Kaliningrad, Russia.
- Department of Materials Technology of Electronics, National University of Science and Technology «MISIS», 119049 Moscow, Russia.
ORCID-Profile: Valeria Kolesnikova, Alexander Omelyanchik, Valeria Rodionova
Förderung
- Immanuel Kant Baltic Federal University
Zitieren
APA
Kolesnikova, V., Baraban, I., Omelyanchik, A., Panina, L., & Rodionova, V. (2024). The Interplay of Core Diameter and Diameter Ratio on the Magnetic Properties of Bistable Glass-Coated Microwires. Micromachines, 15(11), 1284. https://doi.org/10.3390/mi15111284
Vancouver
Kolesnikova V, Baraban I, Omelyanchik A, Panina L, Rodionova V. The Interplay of Core Diameter and Diameter Ratio on the Magnetic Properties of Bistable Glass-Coated Microwires. Micromachines. 2024;15(11):1284. doi:10.3390/mi15111284
BibTeX
@article{Kolesnikova2024,
author = {Kolesnikova, Valeria and Baraban, Irina and Omelyanchik, Alexander and Panina, Larissa and Rodionova, Valeria},
title = {The Interplay of Core Diameter and Diameter Ratio on the Magnetic Properties of Bistable Glass-Coated Microwires},
journal = {Micromachines},
year = {2024},
volume = {15},
number = {11},
pages = {1284},
doi = {10.3390/mi15111284}
}