EUVIMEDEUVIMED entdecken
Open Access · CC BY 4.0

Selective Recovery of Lithium from Waste Lithium Aluminosilicate Glass via Mixed Sulfate Roasting and Water Leaching

Lei Liu, Fupeng Liu, Tao Zhang, Jinfa Liao, Feixiong Chen, Jie Liu

Metals · 16.11.2026 · 16 (11) · 1258

DOI: 10.3390/met16111258 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Metals, online erschienen am 16.11.2026. Verfasst von Lei Liu und 5 weiteren Autor:innen. Die Arbeit nennt 31 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Jiangxi Ganpo Talent Plan Innovative High end Talent Project, Natural Science Foundation for Distinguished Young Scholars of Jiangxi Province, Training Plan for Academic and Technical Leaders of Major Disciplines in Jiangxi Province.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Waste lithium aluminosilicate (LAS) glass is a complex secondary resource characterized by high aluminum and high silicon content, posing significant challenges for the selective recovery of lithium. Conventional recycling processes for such materials are often hindered by poor separation selectivity, complex purification steps, and high energy consumption. To address these limitations, this study proposes an integrated process comprising mixed sulfate roasting, water leaching, selective magnesium precipitation, and lithium carbonate crystallization. Under optimal conditions with a mass ratio of m(K2SO4):m(Na2SO4):m (raw material) = 0.5:0.5:1, roasting at 900 °C for 120 min resulted in the conversion of over 97% of lithium into water-soluble lithium-containing sulfate phases, while aluminum and silicon were transformed into insoluble phases, specifically KAlSi2O6 and Na (AlSi3O8). Subsequent water leaching enabled the direct separation of lithium without the use of acids or alkalis. After roasting and water leaching, a lithium leaching efficiency of 97.19% was achieved, whereas the leaching efficiencies of aluminum and silicon were both below 0.01%, demonstrating exceptional separation selectivity. Residual magnesium impurities in the lithium-bearing leachate were effectively removed via sodium hydroxide precipitation. At an optimized pH of 10.18, the magnesium removal efficiency reached 99.05%. Following purification, lithium carbonate was recovered by sodium carbonate precipitation at 95 °C for 60 min, yielding a Li2CO3 precipitation recovery of 95.33%. Based on these stages, the actual overall lithium recovery of the entire process was calculated to be 92.68%. Compared with conventional LAS-processing routes (salt roasting and acid leaching, or CaO-based calcination generating large amounts of solid waste), this process uses only deionized water for leaching, eliminating acid or alkali consumption. Relative to the conventional spodumene route (1100 °C phase transformation + acid or alkali leaching), the roasting temperature is lowered by 200 °C to 900 °C. This novel process offers a sustainable and economically viable pathway for lithium recovery from waste LAS glass, characterized by reduced energy consumption, minimized environmental impact, and enhanced resource utilization.

Förderung

  • Jiangxi Ganpo Talent Plan Innovative High end Talent Project
  • Natural Science Foundation for Distinguished Young Scholars of Jiangxi Province
  • Training Plan for Academic and Technical Leaders of Major Disciplines in Jiangxi Province
  • Major Science and Technology Research Projects in Yichun City
  • Unveiling and commanding project in Jiangxi Province
  • Postdoctoral Innovative Talent Support Program of Shandong Province and Program of Qingjiang Excellent Young Talents
  • Jiangxi Postdoctoral Science Foundation
  • Jiangxi Provincial Key Laboratory of High-Performance Steel and Iron Alloy Materials

Zitieren

APA

Liu, L., Liu, F., Zhang, T., Liao, J., Chen, F., & Liu, J. (2026). Selective Recovery of Lithium from Waste Lithium Aluminosilicate Glass via Mixed Sulfate Roasting and Water Leaching. Metals, 16(11), 1258. https://doi.org/10.3390/met16111258

Vancouver

Liu L, Liu F, Zhang T, Liao J, Chen F, Liu J. Selective Recovery of Lithium from Waste Lithium Aluminosilicate Glass via Mixed Sulfate Roasting and Water Leaching. Metals. 2026;16(11):1258. doi:10.3390/met16111258

BibTeX
@article{Liu2026,
  author = {Liu, Lei and Liu, Fupeng and Zhang, Tao and Liao, Jinfa and Chen, Feixiong and Liu, Jie},
  title = {Selective Recovery of Lithium from Waste Lithium Aluminosilicate Glass via Mixed Sulfate Roasting and Water Leaching},
  journal = {Metals},
  year = {2026},
  volume = {16},
  number = {11},
  pages = {1258},
  doi = {10.3390/met16111258}
}
Kostenlos starten →