Efficient Copper Extraction from a Refractory Slag-Flotation Copper Sulfide Concentrate via Atmospheric Oxygen-Enriched Leaching

Qifan Zhou, Feng Xie, Hao Ma, Haibei Wang

Metals · 13.07.2026 · 16 (7) · 788

DOI: 10.3390/met16070788 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Metals, online erschienen am 13.07.2026. Verfasst von Qifan Zhou und 3 weiteren Autor:innen. Die Arbeit nennt 43 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Shandong Province Key Research and Development Program, National Natural Science Foundation of China, Ministry of Science and Technology of the People's Republic of China.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

The accumulation of low-grade, refractory copper sulfide concentrates from secondary resources, such as smelting slag-flotation products, represents a growing challenge in the copper industry. This study develops and validates an atmospheric oxygen-enriched leaching process that requires neither grinding nor high pressure, targeting a typical slag-flotation copper sulfide concentrate. Systematic mineralogical analysis shows that copper is 95% in secondary sulfides, with quartz, chlorite, and muscovite as major gangue. Batch leaching optimization identifies the following conditions: H2SO4 250 g/L, temperature 90 °C, leaching time 8–12 h, pulp density 30–33% solids, and oxygen-enriched air (80–90% O2) at a flow rate ensuring sufficient oxygen mass transfer. Under these conditions, copper extraction reaches 97–99% without grinding. Continuous pilot-scale trials (over 500 kg dry feed) compare a five-stage mechanically agitated tank train and a four-stage tower reactor. The tank train achieves a stable copper extraction of 97.1% with a residue grade of 0.53% Cu at 8 h residence time and acid consumption of 857 kg/t concentrate, significantly outperforming the tower reactor. Reducing oxygen purity from 100% to 90% has no measurable effect on extraction, while 80% O2 gives only a 2% loss. The process eliminates grinding, operates at ambient pressure, and uses widely available reactor technology, offering a potentially low-capital and technically robust solution for recovering copper from such refractory secondary sulfide concentrates.

Förderung

  • Shandong Province Key Research and Development Program
  • National Natural Science Foundation of China
  • Ministry of Science and Technology of the People's Republic of China

Zitieren

APA

Zhou, Q., Xie, F., Ma, H., & Wang, H. (2026). Efficient Copper Extraction from a Refractory Slag-Flotation Copper Sulfide Concentrate via Atmospheric Oxygen-Enriched Leaching. Metals, 16(7), 788. https://doi.org/10.3390/met16070788

Vancouver

Zhou Q, Xie F, Ma H, Wang H. Efficient Copper Extraction from a Refractory Slag-Flotation Copper Sulfide Concentrate via Atmospheric Oxygen-Enriched Leaching. Metals. 2026;16(7):788. doi:10.3390/met16070788

BibTeX
@article{Zhou2026,
  author = {Zhou, Qifan and Xie, Feng and Ma, Hao and Wang, Haibei},
  title = {Efficient Copper Extraction from a Refractory Slag-Flotation Copper Sulfide Concentrate via Atmospheric Oxygen-Enriched Leaching},
  journal = {Metals},
  year = {2026},
  volume = {16},
  number = {7},
  pages = {788},
  doi = {10.3390/met16070788}
}
Kostenlos starten →