Effect of Post-Heat Treatment Process on the Microstructure and Mechanical Properties of TA15 Titanium Alloy Fabricated by L-PBF

Zijie Zhang, Shujing Lu, Jiaming Yin, Peng Gao, Liang Zhang, Runguang Li, Shilei Li

Metals · 27.06.2026 · 16 (7) · 708

DOI: 10.3390/met16070708 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Metals, online erschienen am 27.06.2026. Verfasst von Zijie Zhang und 6 weiteren Autor:innen. Die Arbeit wurde bisher 2-mal zitiert (Crossref) und nennt 38 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: National Key Research and Development Program of China, Fundamental Research Funds for the Central Universities.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

TA15 titanium alloy fabricated by Laser Powder Bed Fusion (L-PBF) exhibits high strength but poor ductility due to its fine acicular α′ martensitic microstructure. This study systematically investigates the effects of post-annealing treatments (800–950 °C for 0.5–4 h) on the microstructural evolution and mechanical performance of L-PBF-built TA15. Results show that with increasing temperature and time, the metastable α′ martensite decomposes into a progressively coarser lamellar (α + β) structure. This transformation leads to a decrease in strength and hardness but a significant improvement in ductility, with elongation increasing from (8.5 ± 0.5)% (as-built) to (19.4 ± 1.1)% (900 °C/2 h) as the ultimate tensile strength (UTS) decreased from (1100 ± 29) to (895 ± 37) MPa. However, annealing at 950 °C, which approaches the β-transus temperature, induces a coarse Widmanstätten structure in the alloy. Although this structure yields a relatively high elongation (23.8 ± 3)%, it also leads to excessive strength loss, with an ultimate tensile strength of only (833 ± 23) MPa, rendering it less desirable for structural applications requiring high load-bearing capacity. Moreover, such coarse lamellar structures are generally associated with poor fatigue resistance, as cracks tend to propagate along prior β grain boundaries. An optimal strength-ductility synergy is achieved by annealing at 900 °C for 0.5 h, yielding an ultimate tensile strength of (951 ± 13) MPa and an elongation of (18.8 ± 1.7)%. These findings provide crucial guidance for tailoring the mechanical properties of L-PBF-fabricated TA15 alloy through post-processing heat treatments.

Förderung

  • National Key Research and Development Program of China
  • Fundamental Research Funds for the Central Universities

Zitieren

APA

Zhang, Z., Lu, S., Yin, J., Gao, P., Zhang, L., Li, R., & Li, S. (2026). Effect of Post-Heat Treatment Process on the Microstructure and Mechanical Properties of TA15 Titanium Alloy Fabricated by L-PBF. Metals, 16(7), 708. https://doi.org/10.3390/met16070708

Vancouver

Zhang Z, Lu S, Yin J, Gao P, Zhang L, Li R, et al. Effect of Post-Heat Treatment Process on the Microstructure and Mechanical Properties of TA15 Titanium Alloy Fabricated by L-PBF. Metals. 2026;16(7):708. doi:10.3390/met16070708

BibTeX
@article{Zhang2026,
  author = {Zhang, Zijie and Lu, Shujing and Yin, Jiaming and Gao, Peng and Zhang, Liang and Li, Runguang and Li, Shilei},
  title = {Effect of Post-Heat Treatment Process on the Microstructure and Mechanical Properties of TA15 Titanium Alloy Fabricated by L-PBF},
  journal = {Metals},
  year = {2026},
  volume = {16},
  number = {7},
  pages = {708},
  doi = {10.3390/met16070708}
}
Kostenlos starten →