EUVIMEDEUVIMED entdecken
Open Access · CC BY 4.0

Effect of Post-Weld Heat Treatment on Microstructure and Mechanical Properties of Friction-Stir-Welded Al–Cu–Li Alloy

Ben Lin, Ying Li, Xiwu Li, Yongan Zhang, Kai Wen, Changlin Li, Lizhen Yan, Yanan Li, Hongwei Yan, Zhihui Li, Baiqing Xiong

Metals · 20.05.2026 · 16 (5) · 556

DOI: 10.3390/met16050556 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Metals, online erschienen am 20.05.2026. Verfasst von Ben Lin und 10 weiteren Autor:innen. Die Arbeit nennt 38 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0).

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

To address the insufficient strength of friction-stir-welded (FSW) ultra-high-strength Al–Cu–Li alloy joints, the effects of post-weld heat treatment (PWHT) on microstructural evolution and mechanical properties were systematically investigated. The as-welded joint showed a “W”-shaped microhardness profile, with the minimum value located in the thermo-mechanically affected zone (TMAZ), mainly caused by the dissolution of T1 phases and precipitation of coarse AlCu, AlCuMg, and AlCuMn phases during welding. Direct artificial aging at 155 °C for 24 h failed to improve joint strength due to solute depletion induced by pre-existing coarse secondary phases. Solution treatment re-dissolved coarse precipitates into the matrix, and subsequent aging led to uniform precipitation dominated by T1 and θ′ phases, with a consistent microhardness of ~155 HV across all zones. By introducing pre-stretching deformation after solution treatment, T1 became the dominant strengthening phase in all regions, accompanied by a remarkable increase in both microhardness and tensile strength. With 3% pre-stretching, the microhardness reached 185 HV, and the ultimate tensile strength of the joint reached 600 MPa, corresponding to a joint efficiency as high as 95%, which is superior to most reported values for Al–Li alloy FSW joints. This study clarifies the precipitation evolution mechanism under tailored PWHT and provides an effective strategy for property regulation of high-performance Al–Cu–Li alloy FSW structures in aerospace applications.

Zitieren

APA

Lin, B., Li, Y., Li, X., Zhang, Y., Wen, K., Li, C., Yan, L., Li, Y., Yan, H., Li, Z., & Xiong, B. (2026). Effect of Post-Weld Heat Treatment on Microstructure and Mechanical Properties of Friction-Stir-Welded Al–Cu–Li Alloy. Metals, 16(5), 556. https://doi.org/10.3390/met16050556

Vancouver

Lin B, Li Y, Li X, Zhang Y, Wen K, Li C, et al. Effect of Post-Weld Heat Treatment on Microstructure and Mechanical Properties of Friction-Stir-Welded Al–Cu–Li Alloy. Metals. 2026;16(5):556. doi:10.3390/met16050556

BibTeX
@article{Lin2026,
  author = {Lin, Ben and Li, Ying and Li, Xiwu and Zhang, Yongan and Wen, Kai and Li, Changlin and Yan, Lizhen and Li, Yanan and Yan, Hongwei and Li, Zhihui and Xiong, Baiqing},
  title = {Effect of Post-Weld Heat Treatment on Microstructure and Mechanical Properties of Friction-Stir-Welded Al–Cu–Li Alloy},
  journal = {Metals},
  year = {2026},
  volume = {16},
  number = {5},
  pages = {556},
  doi = {10.3390/met16050556}
}
Kostenlos starten →