Shrinkage Depression Formation and Yield of Ti–48 at.% Al–2 at.% Nb–2 at.% Cr Ingots Produced by Bottom-Pouring Cold Crucible Induction Melting
Metals · 28.04.2026 · 16 (5) · 477
DOI: 10.3390/met16050477 ↗Kurz gefasst
Fachartikel in der Zeitschrift Metals, online erschienen am 28.04.2026. Verfasst von Tomohiro Nishimura und 6 weiteren Autor:innen. Die Arbeit nennt 23 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Council for Science, Technology and Innovation.
Themen: Depression
Abstract (Originalsprache)
In this study, a Ti–48 at.% Al–2 at.% Nb–2 at.% Cr alloy was cast by bottom-pouring cold crucible induction melting (CCIM), and the shrinkage depressions formed in ingots during solidification were investigated. Ingots with different heights were produced, and shrinkage depression height and yield were evaluated based on longitudinal cross-sectional observations. The normalized ingot height ranged from 4 to 25, and the shrinkage depression height increased from 20 mm to 105 mm with increasing ingot height. The yield ranged from 77% to 97% and did not increase monotonically, exhibiting noticeable scatter even among ingots with similar heights. The casting rate ranged from 0.025 kg/s to 0.18 kg/s, and the shrinkage depression height increased with increasing casting rate, whereas no clear correlation was observed between the yield and the casting rate. When the nozzle inner diameter ranged from 2 mm to 5 mm, both the shrinkage depression height and the yield increased, accompanied by scatter. The Reynolds number was evaluated as a parameter representing the average flow condition of the pouring stream; however, shrinkage depression formation could not be uniquely explained by the Reynolds number alone, indicating that melt feeding behavior and heat extraction conditions must also be considered.
Förderung
- Council for Science, Technology and Innovation
Zitieren
APA
Nishimura, T., Matsuwaka, D., Ishida, H., Nohara, M., Nakamura, T., Yamada, Y., & Shoji, A. (2026). Shrinkage Depression Formation and Yield of Ti–48 at.% Al–2 at.% Nb–2 at.% Cr Ingots Produced by Bottom-Pouring Cold Crucible Induction Melting. Metals, 16(5), 477. https://doi.org/10.3390/met16050477
Vancouver
Nishimura T, Matsuwaka D, Ishida H, Nohara M, Nakamura T, Yamada Y, et al. Shrinkage Depression Formation and Yield of Ti–48 at.% Al–2 at.% Nb–2 at.% Cr Ingots Produced by Bottom-Pouring Cold Crucible Induction Melting. Metals. 2026;16(5):477. doi:10.3390/met16050477
BibTeX
@article{Nishimura2026,
author = {Nishimura, Tomohiro and Matsuwaka, Daisuke and Ishida, Hitoshi and Nohara, Masami and Nakamura, Tetsuya and Yamada, Yusuke and Shoji, Aoi},
title = {Shrinkage Depression Formation and Yield of Ti–48 at.% Al–2 at.% Nb–2 at.% Cr Ingots Produced by Bottom-Pouring Cold Crucible Induction Melting},
journal = {Metals},
year = {2026},
volume = {16},
number = {5},
pages = {477},
doi = {10.3390/met16050477}
}
EUVIMED