EUVIMEDEUVIMED entdecken
Open Access · CC BY 4.0

Study on Growth Mechanism and Characteristics of Zirconium Alloy Micro-Arc Oxidation Film

Mingli Wang, Kai Lv, Zhaoxin Du, Weidong Chen, Pengfei Ji, Wei Wang, Zhi Pang

Metals · 11.05.2023 · 13 (5) · 935

DOI: 10.3390/met13050935 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Metals, online erschienen am 11.05.2023. Verfasst von Mingli Wang und 6 weiteren Autor:innen. Die Arbeit wurde bisher 16-mal zitiert (Crossref) und nennt 21 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: University Science Foundation for Young Science and Technology Talents in Inner Mongolia Autonomous Region of China, Research Funds for Universities of Autonomous Region, National Natural Science Foundation of China.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Ceramic coatings on R60705 zirconium alloy were prepared on the surface by the micro-arc oxidation (MAO) technique in electrolytes containing Na2SiO3, NaOH, and Na2EDTA. The growth behavior of the MAO ceramic coatings at different stages, including growth rate, microstructure, and phase composition, was investigated using the method of direct observation of the boundary area. The results showed that the growth of the MAO coatings on R60705 zirconium alloy occurred in both inward and outward directions. At an oxidation time of 5 min, the thickness of the oxidation layer increased fastest, reaching 103.43 μm, with a growth rate of 0.345 μm/s. After 5 min, the growth rate decreased and tended to level off around 15 min, with a thickness and growth rate of 162.7 μm and 0.181 μm/s, respectively. The total thickness of the coatings continuously increased throughout the process, with the outward growth thickness always higher than the inward growth thickness. The composition of the zirconium alloy micro-arc oxidation coatings mainly consisted of monoclinic zirconia (m-ZrO2), tetragonal zirconia (t-ZrO2), and a small amount of SiO2. The main elements in the coatings were Zr, O, and Si. The corrosion resistance of the zirconium alloy micro-arc oxidation coatings increased first and then decreased with increasing oxidation time, with a corrosion current density of 8.876 × 10−9 A·cm−2 at 15 min, indicating the best corrosion resistance.

Förderung

  • University Science Foundation for Young Science and Technology Talents in Inner Mongolia Autonomous Region of China
  • Research Funds for Universities of Autonomous Region
  • National Natural Science Foundation of China
  • Inner Mongolia Natural Science Foundation

Zitieren

APA

Wang, M., Lv, K., Du, Z., Chen, W., Ji, P., Wang, W., & Pang, Z. (2023). Study on Growth Mechanism and Characteristics of Zirconium Alloy Micro-Arc Oxidation Film. Metals, 13(5), 935. https://doi.org/10.3390/met13050935

Vancouver

Wang M, Lv K, Du Z, Chen W, Ji P, Wang W, et al. Study on Growth Mechanism and Characteristics of Zirconium Alloy Micro-Arc Oxidation Film. Metals. 2023;13(5):935. doi:10.3390/met13050935

BibTeX
@article{Wang2023,
  author = {Wang, Mingli and Lv, Kai and Du, Zhaoxin and Chen, Weidong and Ji, Pengfei and Wang, Wei and Pang, Zhi},
  title = {Study on Growth Mechanism and Characteristics of Zirconium Alloy Micro-Arc Oxidation Film},
  journal = {Metals},
  year = {2023},
  volume = {13},
  number = {5},
  pages = {935},
  doi = {10.3390/met13050935}
}