Utilization of Renewable Carbon in Electric Arc Furnace-Based Steel Production: Comparative Evaluation of Properties of Conventional and Non-Conventional Carbon-Bearing Sources

Lina Kieush, Johannes Schenk, Andrii Koveria, Gerd Rantitsch, Andrii Hrubiak, Horst Hopfinger

Metals · 06.04.2023 · 13 (4) · 722

DOI: 10.3390/met13040722 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Metals, online erschienen am 06.04.2023. Verfasst von Lina Kieush und 5 weiteren Autor:innen. Die Arbeit wurde bisher 29-mal zitiert (Crossref) und nennt 61 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0).

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Conventional (anthracite, calcined petroleum coke, and coke) and non-conventional (biochar, and biocokes (3 wt.% torrefied wood, and 3 wt.% petroleum coke + 3 wt.% charcoal)) carbon-bearing sources have been studied for their use in electric arc furnace (EAF)-based steel production. Commonly, for the use of carbon sources in EAFs, one of the important properties is the content of fixed carbon, the release of volatiles as well as the elemental composition of inorganics. The properties of six carbon sources were analyzed by determining the proximate analysis, X-ray fluorescence analysis (XRF), coke reactivity index (CRI), and strength after reaction with CO2 (CSR), Brunauer–Emmett–Teller (BET) specific surface area and Barrett–Joyner–Halenda (BJH) pore size and volume analysis, ash chemical analysis, optical and scanning microscopy, Raman spectroscopy and X-ray diffraction (XRD) analysis. The results indicate biocoke as a promising option to replace conventional carbon-bearing sources. In the sample set, the fixed carbon, volatiles, and ash content of the biocokes were similar despite the total difference in additives. Additionally, the use of additives did not significantly affect the biocoke reactivity indices, but slightly decreased the strength after the reaction with CO2. Carbon-bearing sources have been characterized in terms of their structural properties. XRD analysis revealed that the amount of disordered carbon increased in the order: coke < calcined petroleum coke ~ biocoke (3 wt.% torrefied wood) < biocoke (3 wt.% petroleum coke + 3 wt.% charcoal) < biochar. The results obtained on the physical, chemical, and structural properties of carbon sources are the basis for further research on the behavior of slag foaming.

Zitieren

APA

Kieush, L., Schenk, J., Koveria, A., Rantitsch, G., Hrubiak, A., & Hopfinger, H. (2023). Utilization of Renewable Carbon in Electric Arc Furnace-Based Steel Production: Comparative Evaluation of Properties of Conventional and Non-Conventional Carbon-Bearing Sources. Metals, 13(4), 722. https://doi.org/10.3390/met13040722

Vancouver

Kieush L, Schenk J, Koveria A, Rantitsch G, Hrubiak A, Hopfinger H. Utilization of Renewable Carbon in Electric Arc Furnace-Based Steel Production: Comparative Evaluation of Properties of Conventional and Non-Conventional Carbon-Bearing Sources. Metals. 2023;13(4):722. doi:10.3390/met13040722

BibTeX
@article{Kieush2023,
  author = {Kieush, Lina and Schenk, Johannes and Koveria, Andrii and Rantitsch, Gerd and Hrubiak, Andrii and Hopfinger, Horst},
  title = {Utilization of Renewable Carbon in Electric Arc Furnace-Based Steel Production: Comparative Evaluation of Properties of Conventional and Non-Conventional Carbon-Bearing Sources},
  journal = {Metals},
  year = {2023},
  volume = {13},
  number = {4},
  pages = {722},
  doi = {10.3390/met13040722}
}
Kostenlos starten →