Kurz gefasst

Fachartikel in der Zeitschrift Metals, online erschienen am 17.01.2023. Verfasst von Shanfeng Lao und 11 weiteren Autor:innen. Die Arbeit wurde bisher 6-mal zitiert (Crossref) und nennt 54 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: National key R&D Program of China, Natural Science Foundation of China Youth Foundation Project, Fundamental Research Founds for the Central Universities of Central South University.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Creep aging behavior of a pre-strain and under-age treated 7B04 aluminum alloy (7B04-P for short) was systematically investigated under different temperatures and applied stresses. A lot of dislocation tangles and η’/GPzs were formed in the Al matrix of the 7B04-P al alloy. With the increase in temperature and applied stress, the total creep strain and steady-state creep rate increased significantly. However, the mechanical properties of creep-aged 7B04-P al alloy are sensitive to temperature rather than applied stress. The age-hardening precipitates and grain boundaries change obviously when the temperature rises to 160 °C. Compare to the low temperature (less than 160 °C) creep-aged samples, the size of precipitates is much larger, the width of PFZ is broader, and the grain boundary precipitates are more discontinuous and coarsen. As expected, the electrical conductivity is improved after the high-temperature creep aging process at 160 °C. Last but not least, the creep deformation of 7B04-P al alloy almost retains that of AA7B04-T7451. Meanwhile, the mechanical properties after the creep aging process of 7B04-P al alloy are better than that of AA7B04-T7451. It can be suggested that the novel high-temperature creep age forming of the thermo-mechanical treated 7B04 aluminum alloy can enhance the forming efficiency and comprehensive properties for aerospace industries.

Förderung

  • National key R&D Program of China
  • Natural Science Foundation of China Youth Foundation Project
  • Fundamental Research Founds for the Central Universities of Central South University
  • Hunan Provincial Innovation Foundation for Postgraduate
  • National Natural Science Foundation of China
  • Hunan Natural Science Foundation Youth Foundation Project

Zitieren

APA

Lao, S., Zhan, L., Qian, W., Xu, Y., Ma, B., Liu, C., Huang, M., Yang, Y., Chen, K., Peng, N., Gao, T., & Xi, H. (2023). Creep Aging Behavior of a Thermo-Mechanical Treated 7B04 Aluminum Alloy. Metals, 13(2), 182. https://doi.org/10.3390/met13020182

Vancouver

Lao S, Zhan L, Qian W, Xu Y, Ma B, Liu C, et al. Creep Aging Behavior of a Thermo-Mechanical Treated 7B04 Aluminum Alloy. Metals. 2023;13(2):182. doi:10.3390/met13020182

BibTeX
@article{Lao2023,
  author = {Lao, Shanfeng and Zhan, Lihua and Qian, Wei and Xu, Yongqian and Ma, Bolin and Liu, Chuhui and Huang, Minghui and Yang, Youliang and Chen, Kuigen and Peng, Nanhui and Gao, Tuanjie and Xi, Hongfei},
  title = {Creep Aging Behavior of a Thermo-Mechanical Treated 7B04 Aluminum Alloy},
  journal = {Metals},
  year = {2023},
  volume = {13},
  number = {2},
  pages = {182},
  doi = {10.3390/met13020182}
}
Kostenlos starten →