Fachartikel in der Zeitschrift Membranes, online erschienen am 17.03.2023. Verfasst von Eveline Kuhnert und 4 weiteren Autor:innen. Beteiligte Einrichtung: Institute of Chemical Engineering and Environmental Technology, Graz University of Technology, Inffeldgasse 25/C, 8010 Graz, Austria. Die Arbeit wurde bisher 69-mal zitiert (Crossref) und nennt 44 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Austrian Research Promotion Agency, the Austrian Research Promotion Agency (FFG), the TU Graz Open Access Publishing Fund.

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Polymer electrolyte membrane water electrolysis (PEMWE) is a leading candidate for the development of a sustainable hydrogen infrastructure. The heart of a PEMWE cell is represented by the membrane electrode assembly (MEA), which consists of a polymer electrolyte membrane (PEM) with catalyst layers (CLs), flow fields, and bipolar plates (BPPs). The weakest component of the system is the PEM, as it is prone to chemical and mechanical degradation. Membrane chemical degradation is associated with the formation of hydrogen peroxide due to the crossover of product gases (H2 and O2). In this paper, membrane failure due to H2 crossover was addressed in a membrane-focused accelerated stress test (AST). Asymmetric H2O and gas supply were applied to a test cell in OCV mode at two temperatures (60 °C and 80 °C). Electrochemical characterization at the beginning and at the end of testing revealed a 1.6-fold higher increase in the high-frequency resistance (HFR) at 80 °C. The hydrogen crossover was measured with a micro-GC, and the fluoride emission rate (FER) was monitored during the ASTs. A direct correlation between the FER and H2 crossover was identified, and accelerated membrane degradation at higher temperatures was detected.

Schlagwörter

Stichwörter der Autor:innen

accelerated stress test (AST)fluoride emission rate (FER)hydrogen crossovermembrane degradationpolymer electrolyte membrane water electrolysis (PEMWE)

Autor:innen und Institutionen

  • Institute of Chemical Engineering and Environmental Technology, Graz University of Technology, Inffeldgasse 25/C, 8010 Graz, Austria.
  • AiDEXA GmbH, Bergmanngasse 45/10, 8010 Graz, Austria.

ORCID-Profile: Eveline Kuhnert, Mathias Heidinger, Viktor Hacker, Merit Bodner

Förderung

  • Austrian Research Promotion Agency
  • the Austrian Research Promotion Agency (FFG)
  • the TU Graz Open Access Publishing Fund

Zitieren

APA

Kuhnert, E., Heidinger, M., Sandu, D., Hacker, V., & Bodner, M. (2023). Analysis of PEM Water Electrolyzer Failure Due to Induced Hydrogen Crossover in Catalyst-Coated PFSA Membranes. Membranes, 13(3), 348. https://doi.org/10.3390/membranes13030348

Vancouver

Kuhnert E, Heidinger M, Sandu D, Hacker V, Bodner M. Analysis of PEM Water Electrolyzer Failure Due to Induced Hydrogen Crossover in Catalyst-Coated PFSA Membranes. Membranes. 2023;13(3):348. doi:10.3390/membranes13030348

BibTeX
@article{Kuhnert2023,
  author = {Kuhnert, Eveline and Heidinger, Mathias and Sandu, Daniel and Hacker, Viktor and Bodner, Merit},
  title = {Analysis of PEM Water Electrolyzer Failure Due to Induced Hydrogen Crossover in Catalyst-Coated PFSA Membranes},
  journal = {Membranes},
  year = {2023},
  volume = {13},
  number = {3},
  pages = {348},
  doi = {10.3390/membranes13030348}
}
Kostenlos starten →