Alkali-Activated Mortars from Municipal Solid Waste Incineration Bottom Ash: Optimisation of NaOH Molarity and Curing Temperature by Response Surface Methodology
Materials · 21.11.2026 · 19 (23) · 4943
DOI: 10.3390/ma19234943 ↗Kurz gefasst
Fachartikel in der Zeitschrift Materials, online erschienen am 21.11.2026. Verfasst von Katarzyna Kalinowska-Wichrowska und 6 weiteren Autor:innen. Die Arbeit nennt 22 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Polish Ministry of Science.
Abstract (Originalsprache)
Municipal solid waste incineration bottom ash (MSWI BA) is an abundant mineral residue whose valorisation as a precursor for alkali-activated binders supports circular-economy objectives. This study investigates cement-free alkali-activated mortars prepared with ground MSWI BA (8/16 mm fraction), CEN standard sand and sodium hydroxide (NaOH) solution. A central composite design (CCD) with two factors—curing temperature (45–105 °C) and NaOH molarity (4–12 M, at a constant activator-solution mass)—and ten series (four factorial, four axial and two centre points) was used to model the 28-day flexural strength, compressive strength and water absorption. The MSWI BA was characterised by X-ray fluorescence (XRF), X-ray diffraction (XRD), scanning electron microscopy (SEM), laser granulometry and the Chapelle pozzolanic-activity test. The ground ash (mean particle size ≈8 µm, Blaine specific surface area 491 m2/kg, Chapelle pozzolanic activity 547 mg Ca(OH)2/g) consisted mainly of quartz and anorthite with a pronounced amorphous phase. The highest 28-day compressive strength (22.9 MPa) and flexural strength (5.50 MPa) were measured at 60 °C and 6 M NaOH, whereas the lowest water absorption (7.89%) was obtained at 75 °C and 4 M NaOH; excessive molarity (12 M) and temperature extremes (45 and 105 °C) deteriorated the hardened matrix. Second-order response surface models fitted to the ten batch means (R2 = 0.81–0.93) located a model-based optimum near 70–75 °C and 5–6 M NaOH; with the batch as the experimental unit, however, the model was statistically significant only for flexural strength (F(5,4) = 10.03, p = 0.022). Three independent confirmation batches prepared at 72.5 °C and 5.5 M NaOH reproduced the predicted properties closely (measured 21.7 MPa compressive strength, 5.3 MPa flexural strength and 7.6% water absorption versus predicted 21.9 MPa, 5.2 MPa and 8.0%), validating the model-based optimum. The results show that MSWI BA has promising mechanical potential for non-structural cement-free mortars, subject to environmental and durability assessments.
Förderung
- Polish Ministry of Science
Zitieren
APA
Kalinowska-Wichrowska, K., Granatyr, K., Kosior-Kazberuk, M., Masłoń, A., Malaiškienė, J., Baluta, K., & Skorbiłowicz, J. (2026). Alkali-Activated Mortars from Municipal Solid Waste Incineration Bottom Ash: Optimisation of NaOH Molarity and Curing Temperature by Response Surface Methodology. Materials, 19(23), 4943. https://doi.org/10.3390/ma19234943
Vancouver
Kalinowska-Wichrowska K, Granatyr K, Kosior-Kazberuk M, Masłoń A, Malaiškienė J, Baluta K, et al. Alkali-Activated Mortars from Municipal Solid Waste Incineration Bottom Ash: Optimisation of NaOH Molarity and Curing Temperature by Response Surface Methodology. Materials. 2026;19(23):4943. doi:10.3390/ma19234943
BibTeX
@article{KalinowskaWichrowska2026,
author = {Kalinowska-Wichrowska, Katarzyna and Granatyr, Krzysztof and Kosior-Kazberuk, Marta and Masłoń, Adam and Malaiškienė, Jurgita and Baluta, Karolina and Skorbiłowicz, Julia},
title = {Alkali-Activated Mortars from Municipal Solid Waste Incineration Bottom Ash: Optimisation of NaOH Molarity and Curing Temperature by Response Surface Methodology},
journal = {Materials},
year = {2026},
volume = {19},
number = {23},
pages = {4943},
doi = {10.3390/ma19234943}
}