Microstructural Evolution and Compressive Strength Degradation of Hydraulic Asphalt Concrete Under Extreme Freeze–Thaw Cycles

Xubin Huang, Zhe Miao, Guangshan Shi, Yongzhi Liu, Shengting Wang, Shuangchao Lei, Xiangyang Li, Jiansheng Wang

Materials · 11.11.2026 · 19 (22) · 4783

DOI: 10.3390/ma19224783 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Materials, online erschienen am 11.11.2026. Verfasst von Xubin Huang und 7 weiteren Autor:innen. Die Arbeit nennt 43 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Open Fund of the State Key Laboratory of Cryospheric Science and Frozen Soil Engineering.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Driven by China’s carbon peaking and carbon neutrality goals, pumped-storage hydropower projects have developed rapidly, while power stations in Northwest China face challenges posed by extreme temperature conditions. Unlike previous studies on asphalt mixtures under conventional freeze–thaw conditions, this study employs multiscale characterization methods to investigate the deterioration behavior of dense-graded hydraulic asphalt concrete under extreme temperature cycling. SBS-modified asphalt concrete specimens were vacuum-saturated and subjected to 0, 5, 10, 15, and 20 accelerated freeze–thaw cycles over a temperature range from −45 to + 60 °C. Uniaxial compression tests, relative mass change measurements, MIP, CT with three-dimensional pore reconstruction, and SEM were employed. The results show that compressive strength gradually decreased with increasing freeze–thaw cycles, while mercury-accessible pore volume, relative mass change, and interfacial defects progressively increased. After 20 cycles, compressive strength decreased by 9.29%, while the mercury-accessible volume of large capillary pores increased by 19.05%. SEM observations of the selected fields revealed more pronounced pores and cracks near the aggregate–asphalt mastic interface. These findings suggest that the aggregate–asphalt mastic interface is one of the relatively vulnerable regions under extreme cyclic exposure, although changes in the asphalt binder itself may also contribute to material deterioration. This study provides experimental evidence for understanding the deterioration behavior of hydraulic asphalt concrete under extreme temperature conditions.

Förderung

  • Open Fund of the State Key Laboratory of Cryospheric Science and Frozen Soil Engineering

Zitieren

APA

Huang, X., Miao, Z., Shi, G., Liu, Y., Wang, S., Lei, S., Li, X., & Wang, J. (2026). Microstructural Evolution and Compressive Strength Degradation of Hydraulic Asphalt Concrete Under Extreme Freeze–Thaw Cycles. Materials, 19(22), 4783. https://doi.org/10.3390/ma19224783

Vancouver

Huang X, Miao Z, Shi G, Liu Y, Wang S, Lei S, et al. Microstructural Evolution and Compressive Strength Degradation of Hydraulic Asphalt Concrete Under Extreme Freeze–Thaw Cycles. Materials. 2026;19(22):4783. doi:10.3390/ma19224783

BibTeX
@article{Huang2026,
  author = {Huang, Xubin and Miao, Zhe and Shi, Guangshan and Liu, Yongzhi and Wang, Shengting and Lei, Shuangchao and Li, Xiangyang and Wang, Jiansheng},
  title = {Microstructural Evolution and Compressive Strength Degradation of Hydraulic Asphalt Concrete Under Extreme Freeze–Thaw Cycles},
  journal = {Materials},
  year = {2026},
  volume = {19},
  number = {22},
  pages = {4783},
  doi = {10.3390/ma19224783}
}
Kostenlos starten →