Laser-Assisted Wafering of 4H-SiC: From Subsurface Modification and Crack Coalescence to Controlled Separation
Materials · 03.11.2026 · 19 (21) · 4688
DOI: 10.3390/ma19214688 ↗Kurz gefasst
Übersichtsarbeit in der Zeitschrift Materials, online erschienen am 03.11.2026. Verfasst von Zhiqiang Fan und 2 weiteren Autor:innen. Beteiligte Einrichtung: School of Mechanics and Transportation Engineering, Northwestern Polytechnical University, Xi'an 710072, China. Die Arbeit nennt 55 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: National Key Research and Development Program of China, Natural Science Basic Research Program of Shaanxi.
Abstract (Originalsprache)
Laser-assisted wafering can reduce material consumption in silicon carbide (SiC) substrate manufacturing, but successful subsurface modification does not, by itself, guarantee controlled wafer release. This review treats 4H-SiC wafering as a two-step process comprising laser formation of a weakened subsurface layer, followed by assisted separation. We connect nonlinear energy deposition, phase transformation and residual stress to crack nucleation, interaction and coalescence, and then assess mechanical and ultrasonic separation, polymer-assisted cold splitting, continuous-wave laser splitting, other thermal-stress routes, and chemical or hybrid release within a common fracture-mechanics framework. Reported results show that crystallographic orientation, scan arrangement, crack coplanarity, acoustic coupling and liquid medium strongly affect separation. Nominal separation stress, residual stripping force and internally generated thermal stress are distinct metrics and should not be compared directly. Reported separation strengths span more than three orders of magnitude, from above 38 MPa to about 0.04 MPa, primarily because laser processing produces very different crack-network connectivity. As-split roughness ranges from about 0.16 to 6.5 µm and is governed mainly by the laser step and 4° off-cut geometry. Joint optimization of modification and separation, together with standardized reporting, is therefore essential for scalable low-loss wafering.
Schlagwörter
Stichwörter der Autor:innen
Autor:innen und Institutionen
- School of Mechanics and Transportation Engineering, Northwestern Polytechnical University, Xi'an 710072, China.
- The Second Research Institute of China Electronics Technology Group Corporation, Taiyuan 030024, China.
ORCID-Profile: Pengsen Zhang, Beichen Hu
Förderung
- National Key Research and Development Program of China
- Natural Science Basic Research Program of Shaanxi
Zitieren
APA
Fan, Z., Zhang, P., & Hu, B. (2026). Laser-Assisted Wafering of 4H-SiC: From Subsurface Modification and Crack Coalescence to Controlled Separation. Materials, 19(21), 4688. https://doi.org/10.3390/ma19214688
Vancouver
Fan Z, Zhang P, Hu B. Laser-Assisted Wafering of 4H-SiC: From Subsurface Modification and Crack Coalescence to Controlled Separation. Materials. 2026;19(21):4688. doi:10.3390/ma19214688
BibTeX
@article{Fan2026,
author = {Fan, Zhiqiang and Zhang, Pengsen and Hu, Beichen},
title = {Laser-Assisted Wafering of 4H-SiC: From Subsurface Modification and Crack Coalescence to Controlled Separation},
journal = {Materials},
year = {2026},
volume = {19},
number = {21},
pages = {4688},
doi = {10.3390/ma19214688}
}
EUVIMED