Strain-Dependent High-Temperature Low-Cycle Fatigue Behavior and Damage Mechanisms of GH4169 Alloy After Cold-Drawing Pre-Deformation and Short-Time Annealing

Haiquan Liu, Xinyu Gu, Senhao Yang iD, Ting Xiong, Yanzhong Tian iD, Meng Wang iD, Feng Liu

Materials · 31.10.2026 · 19 (21) · 4649

DOI: 10.3390/ma19214649 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Materials, online erschienen am 31.10.2026. Verfasst von Haiquan Liu und 6 weiteren Autor:innen. Beteiligte Einrichtung: Testing Center, Ji Hua Laboratory, Foshan 528200, China. Die Arbeit nennt 38 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: National Natural Science Foundation of China, GuangDong Basic and Applied Basic Research Foundation, Basic and research Project of Guangzhou.

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

The high-temperature low-cycle fatigue (LCF) response of GH4169 (Inconel 718) is sensitive to the initial microstructural state, yet the coupled effects of cold-drawing pre-deformation and subsequent annealing remain insufficiently understood. A direct-aged condition was used as the reference, while specimens subjected to 14% and 20% cold drawing were tested either without annealing (Z) or after short-time annealing at 930 °C for 10 min (T). Strain-controlled LCF tests were conducted at 650 °C at total strain amplitudes of 0.4%, 0.6%, and 0.8%, with EBSD, SEM, and TEM used to characterize microstructures and fatigue damage. The highest recorded Nf values were 13,679 cycles for 20%-Z at 0.4%, 1095 cycles for the direct-aged reference at 0.6%, and 289 cycles for 20%-T at 0.8%. Retained deformation substructures and low-angle grain boundaries may contribute to local slip accommodation at low strain amplitude. The dislocation structures observed after testing at 0.4% and 0.6% suggest more extensive localized cyclic plasticity at the higher amplitude, while partial recovery after annealing may benefit high-amplitude plastic accommodation. These results suggest that the balance between retained deformation substructures and partial recovery contributes to the strain-amplitude-dependent LCF response of GH4169.

Schlagwörter

Stichwörter der Autor:innen

GH4169 alloycold-drawing pre-deformationlow-cycle fatigueshort-time annealingstrain-amplitude dependence

Autor:innen und Institutionen

  • Testing Center, Ji Hua Laboratory, Foshan 528200, China.
  • Guangdong Provincial Key Laboratory of Advanced Corrosion-Resistant Materials, Institute of Corrosion Science and Technology, Corrosion-Resistant Centre for Light Metal, Guangzhou 510530, China.
  • Institute of Advanced Materials and Technology, Guangdong University of Technology, Guangzhou 510006, China.
  • Key Laboratory for Anisotropy and Texture of Materials (Ministry of Education), School of Materials Science and Engineering, Northeastern University, Shenyang 110819, China.

ORCID-Profile: Senhao Yang, Yanzhong Tian, Meng Wang

Förderung

  • National Natural Science Foundation of China
  • GuangDong Basic and Applied Basic Research Foundation
  • Basic and research Project of Guangzhou
  • Youth S&T Talent Support Programme of Guangdong Provincial Association for Science and Technology
  • Youth S&T Talent Support Programme of Guangdong Provincial Association for Science and Technology

Zitieren

APA

Liu, H., Gu, X., Yang, S., Xiong, T., Tian, Y., Wang, M., & Liu, F. (2026). Strain-Dependent High-Temperature Low-Cycle Fatigue Behavior and Damage Mechanisms of GH4169 Alloy After Cold-Drawing Pre-Deformation and Short-Time Annealing. Materials, 19(21), 4649. https://doi.org/10.3390/ma19214649

Vancouver

Liu H, Gu X, Yang S, Xiong T, Tian Y, Wang M, et al. Strain-Dependent High-Temperature Low-Cycle Fatigue Behavior and Damage Mechanisms of GH4169 Alloy After Cold-Drawing Pre-Deformation and Short-Time Annealing. Materials. 2026;19(21):4649. doi:10.3390/ma19214649

BibTeX
@article{Liu2026,
  author = {Liu, Haiquan and Gu, Xinyu and Yang, Senhao and Xiong, Ting and Tian, Yanzhong and Wang, Meng and Liu, Feng},
  title = {Strain-Dependent High-Temperature Low-Cycle Fatigue Behavior and Damage Mechanisms of GH4169 Alloy After Cold-Drawing Pre-Deformation and Short-Time Annealing},
  journal = {Materials},
  year = {2026},
  volume = {19},
  number = {21},
  pages = {4649},
  doi = {10.3390/ma19214649}
}
Kostenlos starten →